LOCTITE EA 9340

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9340

Main features

  • Visual 1:1 Mix Confirmation
  • Extended 90-Minute Pot Life
  • High-Temperature Shear Retention

Product Description

LOCTITE EA 9340 is a two-part, general-purpose epoxy paste adhesive for bonding wood, metals, ceramics and most plastics where heat and chemical exposure are important. Part A and Part B mix 1:1 by weight or volume to a uniform gray paste, with a 90-minute pot life for a 100 g mass at 25 deg C. Handling strength develops in 6 to 8 hours at room temperature, and full cure can be reached in 24 hours at 25 deg C or accelerated with heat. The cured adhesive can be sanded, drilled and painted for finish work.

Key features

  • Visual 1:1 mixing: Green Part A and gray Part B mix 1:1 to a uniform gray paste.
  • Extended pot life: The mixed adhesive has a 90-minute pot life for a 100 g mass at 25 deg C.
  • High-temperature shear retention: Typical shear strength is 1,850 psi at 82 deg C after the stated cure on etched aluminum.

Applications

Applications include bonding wood, metals, ceramics and most plastics for general-purpose assemblies requiring heat and chemical resistance.

Product Family

LOCTITE EA 9340

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Green / Grey
Component System
Two (A / B)
Mix Ratio
1:1

Additional Information

Technical properties

As-supplied properties

Typical component and mixed-system values at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
Part A colorGreenAs supplied
Part B colorGrayAs supplied
Mixed colorGrayAfter complete mixing
ViscosityPastePart A, Part B and mixed system
Mix ratio1:1By weight or by volume
Pot life90minutes100 g mass at 25 deg C
Recommended storage range8 to 21deg CUnopened container in a cool, dry location
Technical properties

Final-state properties

Typical values after 3 days at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
Shore hardnessGreater than 80Durometer DCured material
Shear strength2,100psiASTM D 1002, etched aluminum, tested at -40 deg F
Shear strength2,300psiASTM D 1002, etched aluminum, tested at 77 deg F
Shear strength1,850psiASTM D 1002, etched aluminum, tested at 180 deg F