LOCTITE EA 9306NA

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9306NA

Main features

  • One-Component, Heat-Curing Epoxy Paste
  • Low-Exotherm Bonding Processing
  • 34.5 MPa Aluminum Lap Shear

Product Description

LOCTITE® EA 9306NA Epoxy Paste Adhesive is a gray, thixotropic, one-component epoxy adhesive that develops bonded-joint performance through heat cure. Its sag-resistant consistency supports controlled placement, while its low-exotherm formulation is suited to bonding processes where heat generation is a concern. The adhesive provides tensile lap shear strength across test temperatures from -55°C to 82°C and is also documented for coil and potting applications.

Key features

  • One-component heat-cure system: Supplied ready to use after warming to room temperature, without component mixing.
  • Sag-resistant thixotropic paste: Supports controlled adhesive placement where flow or movement must be limited.
  • Temperature-dependent bond performance: Typical tensile lap shear strength ranges from 27.6 to 34.5 MPa on phosphoric-acid-anodized 2024-T3 clad aluminum.

Applications / Suitable for

  • Bonding applications requiring sag resistance
  • Bonding processes where low exotherm is important
  • Coil applications
  • Potting applications
Product Family

LOCTITE EA 9306NA

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
500,000 to 1,300,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, one-component adhesive. Viscosity values retain the documented test temperature and Brookfield conditions.

Property Value Unit Method / condition
Color Gray — Uncured adhesive
Viscosity 5,000–13,000 Poise 77°F; Brookfield HBT, spindle 7 at 20 rpm
Viscosity 500–1,300 Pa·s 25°C; Brookfield HBT, spindle 7 at 2.1 rad/s
Density 1.35 g/mL Uncured adhesive
Shelf life 1 year; 1 month — 1 year below 40°F/4°C; 1 month below 77°F/25°C

After-processing / final-state properties

Typical cured-material and bonded-joint results. Tensile lap shear values were measured after curing for 1 hour at 270°F/132°C.

Property Value Unit Method / condition
Tensile lap shear strength 4,000 / 27.6 psi / MPa ASTM D1002 at -67°F/-55°C; 2024-T3 clad aluminum, phosphoric-acid anodized per ASTM D3933
Tensile lap shear strength 5,000 / 34.5 psi / MPa ASTM D1002 at 77°F/25°C; 2024-T3 clad aluminum, phosphoric-acid anodized per ASTM D3933
Tensile lap shear strength 4,000 / 27.6 psi / MPa ASTM D1002 at 180°F/82°C; 2024-T3 clad aluminum, phosphoric-acid anodized per ASTM D3933
Approximate service temperature 250 / 121 °F / °C Defined as the temperature at which the adhesive retains 1,000 psi/6.9 MPa using ASTM D1002
Compressive strength 11,000 / 75.8 psi / MPa ASTM D695 at 77°F/25°C; tested using 0.5 in/12.7 mm castings