LOCTITE EA 9017

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9017

Main features

  • Premeasured Resin-Hardener Pack
  • Fast 4-6-Minute Handling
  • Machinable Cured Epoxy Finish

Product Description

LOCTITE EA 9017 is a two-component, room-temperature-curing epoxy adhesive supplied in a premeasured syringe pack for permanent bonding and repair. The clear water-white-to-amber liquid reaches handling strength in 4 to 6 minutes and full cure in 45 to 60 minutes. It bonds metals, ceramics, concrete, wood, glass and most plastics, while the cured material can be drilled, tapped, sanded, machined and painted. Applications include production, maintenance and prototype bonding, plus filling and sealing holes, cracks and worn surfaces.

Key features

  • Premeasured syringe pack: Resin and hardener are supplied in measured quantities for consistent mixing and application.
  • Fast handling and cure: Handling strength develops in 4 to 6 minutes, with full cure in 45 to 60 minutes.
  • Machinable cured epoxy: The cured material can be drilled, tapped, sanded, machined and painted.

Applications

Applications include bonding metals, ceramics, concrete, wood, glass and most plastics, plus repairing, filling and sealing holes, cracks and worn surfaces.

Product Family

LOCTITE EA 9017

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear water white to amber liquid / Translucent
Specific Gravity
1.13 - 1.17
Thermal Properties
Flash Point
>93 °C

Additional Information

Technical properties

As-supplied properties

Typical uncured-product values.

Property Value Unit Method / condition
Chemical typeEpoxy and resinTwo-component system
AppearanceClear water-white to amber liquidUncured
Specific gravity1.13 to 1.17Uncured
Storage range8 to 28deg CUnopened container in a cool, dry location
Technical properties

Final-state properties

Typical cured-product values unless otherwise stated.

Property Value Unit Method / condition
Cured appearanceTranslucentFully cured material
Shear strength2,300psiASTM D 1002
Temperature resistanceUp to 149deg CCured adhesive

Leading Brands Trust in Our Products and Services