LOCTITE EA 7000

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 7000

Main features

  • Dual-Temperature Composite Cure
  • Extended 30-Day Out Time
  • Supported or Unsupported Film

Product Description

LOCTITE EA 7000 AERO is a modified epoxy film adhesive for composite bonding, repair and co-cure assembly. It is available in supported or unsupported constructions, with standard film weights from 0.03 to 0.10 lb/sf and thicknesses from 0.005 to 0.017 in. The green film provides dual-temperature cure capability at 121 deg C or 180 deg C and has an out time greater than 30 days at 32 deg C and 50% relative humidity. Applications include composite repair, composite surfacing, bonding pre-cured composites and co-curing with composite prepregs.

Key features

  • Supported or unsupported film: The modified epoxy film is available with or without a support construction.
  • Dual-temperature cure: The adhesive can be cured at 121 deg C or 180 deg C.
  • Extended out time: Out time is greater than 30 days at 32 deg C and 50% relative humidity.

Applications

Applications include composite repair, composite surfacing, bonding pre-cured composites and co-curing with composite prepregs.

Product Family

LOCTITE EA 7000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Green
Film Thickness
0.127 - 0.38 mm
Physical Properties
Volatiles
<1 %

Additional Information

Technical properties

As-supplied properties

Supplied-film values; configuration-dependent where noted.

Property Value Unit Method / condition
ConstructionSupported or unsupportedModified epoxy film
ScrimNonwoven polyesterOther constructions available on request
Film weight0.03 to 0.10lb/sfMetric range: 146 to 488 g/m^2
Thickness0.005 to 0.017inMetric range: 0.0127 to 0.043 cm
ColorGreenAs supplied
VolatilesLess than 1%As supplied
Out timeGreater than 30daysAt 32 deg C and 50% relative humidity
Shelf lifeGreater than 2yearsAt -18 deg C

Leading Brands Trust in Our Products and Services