LOCTITE EA 608

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE EA 608

Main features

  • Clear Fast-Setting Structural Epoxy
  • 1:1 Weight/Volume Mixing
  • Metal and Plastic Bonding

Product Description

LOCTITE® EA 608 is a clear, two-part, fast-setting epoxy adhesive for structural bonding applications where optical clarity or a short processing time is important. The adhesive mixes at a 1:1 ratio by weight or volume and develops a clear to light-amber appearance after mixing. It has a typical pot life of 5 minutes at 77°F for a 20-gram mixed quantity and reaches handling strength in approximately 10–15 minutes at 77°F, depending on the bond configuration. LOCTITE® EA 608 bonds a variety of metals and plastics and can be fully cured at room temperature or with an accelerated heat cure.

Key features

  • Clear structural bonding: The mixed adhesive cures clear to light amber for assemblies where bondline appearance or optical clarity is important.
  • Fast handling strength: Develops handling strength in approximately 10–15 minutes at 77°F, depending on the bond configuration.
  • Simple 1:1 mixing: Parts A and B are combined at a 1:1 ratio by both weight and volume for cartridge or bulk application.

Applications / Suitable for

  • Structural bonding
  • Bonding metals
  • Bonding plastics
  • Assemblies requiring a clear adhesive bondline

Technical Specifications

General Properties
Color
Milky white / amber / clear or light amber
Mix Ratio
1:1
Pot Life
5 minutes
Specific Gravity
1.16
Physical Properties
Viscosity (Part B)
20000–40000 mPa.s
Thermal Properties
Thermal Conductivity
0.2 W/m.K
Electrical Properties
Dielectric Strength
47 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Mix ratio 1:1 — Part A:Part B, by weight or volume
Pot life 5 min Typical; mixed adhesive, 20-gram quantity at 77°F
Color Milky white / amber / clear to light amber — Part A / Part B / mixed adhesive
Viscosity 200,000–450,000 cP Typical; Part A, ASTM D2393
Viscosity 20,000–40,000 cP Typical; Part B
Specific gravity 1.17 / 1.15 / 1.16 — Typical; Part A / Part B / mixed adhesive

After-processing / final-state properties

Property Value Unit Method / condition
Coefficient of thermal expansion 86 × 10−6 in/in/°C Typical; ASTM D696
Thermal conductivity 5.0 × 10−4 cal·cm/(cm²·s·°C) Typical cured-material value
Hardness 80 Shore D Typical cured-material value
Dielectric strength 1,200 V/mil Typical; ASTM D149
Dielectric constant 3.78 — Typical; 1 kHz, method shown in source as MIL 1-16923
Dissipation factor 2.1 × 10−4 — Typical; ASTM D150 at 1 kHz
Shear strength 2,000 psi Typical; ASTM D1002, etched aluminum, cured 24 hours at 77°F and tested at 77°F
Shear strength 3,000 psi Typical; ASTM D1002, etched aluminum, cured 2 hours at 140°F and tested at 77°F