LOCTITE EA 460

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 460

Main features

  • Low-Odor Low-Bloom Bonding
  • Low-Viscosity Precision Application
  • Rapid Multi-Substrate Fixture

Product Description

LOCTITE 460 is a one-part, low-viscosity alkoxyethyl cyanoacrylate adhesive for rapid bonding of metals, plastics and elastomers. The transparent, colorless-to-straw liquid cures with atmospheric humidity and has a typical cone-and-plate viscosity of 25 to 55 mPa s at 25 deg C. Low odor and low blooming are useful where vapor control is difficult, while fixture develops in less than 5 seconds on several substrates under the stated 22 deg C and 50% relative-humidity conditions. Applications include bonding ABS, PVC, polycarbonate, rubber, wood, paper, leather and fabric.

Key features

  • Low odor and bloom: The alkoxyethyl cyanoacrylate formulation limits odor and visible blooming where vapor control is difficult.
  • Low-viscosity application: Typical cone-and-plate viscosity is 25 to 55 mPa s at 25 deg C.
  • Rapid substrate fixture: Fixture develops in less than 5 seconds on ABS, nitrile rubber, neoprene, phenolic and paper under the stated conditions.

Applications

Applications include rapid bonding of metals, plastics and elastomers, plus porous or absorbent materials such as wood, paper, leather and fabric.

Product Family

LOCTITE EA 460

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent, colorless to straw colored liquid
Specific Gravity
1.1
Physical Properties
Viscosity
25 to 55 mPa.s

Additional Information

Technical properties

As-supplied properties

Typical uncured-product values at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
AppearanceTransparent, colorless to straw-colored liquidUncured
Specific gravity1.1At 25 deg C
Viscosity25 to 55mPa sCone and plate, 25 deg C, shear rate 3,000 s^-1
Viscosity30 to 50mPa sBrookfield LVF, spindle 1, 30 rpm, 25 deg C
Optimal storage range2 to 8deg CUnopened container in a dry location
Technical properties

Final-state properties

Typical bonded-joint values after 72 hours at 22 deg C unless otherwise stated.

Property Value Unit Method / condition
Lap shear strength21N/mm^2ISO 4587, grit-blasted steel
Lap shear strength18N/mm^2ISO 4587, etched aluminum
Lap shear strength7.9N/mm^2ISO 4587, ABS
Lap shear strength7.7N/mm^2ISO 4587, polycarbonate
Block shear strength25N/mm^2ISO 13445, polycarbonate
Tensile strength30N/mm^2ISO 6922, steel pin to steel pin, 24 hours at 22 deg C

Leading Brands Trust in Our Products and Services