LOCTITE EA 3981

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

LOCTITE EA 3981

Main features

  • One-Component No-Mix Adhesive
  • Heat Cure as Low as 100 deg C
  • Disposable-Needle/Syringe/Lancet Cannula Bonding

Product Description

LOCTITE® EA 3981 is a one-component, heat-cure epoxy adhesive developed for assembling disposable medical devices. The translucent, slightly amber liquid requires no mixing and fluoresces under ultraviolet light to support inspection during production. It cures at temperatures as low as 100°C and bonds plastics, metals, and glass. The product is specifically designed for bonding stainless steel cannulae into hubs, syringes, and lancets used in needle assemblies. Its combination of rapid thermal curing, adhesion across multiple substrate types, and resistance to environmental exposure supports high-speed medical-device assembly processes.

Key features

  • One-component epoxy: Requires no mixing before application, simplifying material preparation and dispensing.
  • Rapid heat cure: Cures at temperatures as low as 100°C, with documented cure schedules for production processing.
  • UV fluorescence: Produces a positive response under ultraviolet light to support adhesive-presence inspection.

Applications / Suitable for

  • Bonding stainless steel cannulae into plastic hubs
  • Needle, syringe, and lancet assemblies
  • Assembly of disposable medical devices
  • Bonding plastics, metals, and glass
Product Family

LOCTITE EA 3981

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
One part
Specific Gravity
1.14
Physical Properties
Viscosity
4,000–6,000 mPa.s
Mechanical Properties
Elongation
2.98 %
Chemical Properties
Water Absorption
1.8 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the adhesive before heat curing.

Property Value Unit Method / condition
Technology Epoxy — As supplied
Components One component — Requires no mixing
Appearance Translucent, slightly amber liquid — Uncured material
Fluorescence Positive — Under UV light
Specific gravity 1.14 — At 25°C
Viscosity 4,000–6,000 mPa·s (cP) Brookfield SSA-RVT, 25°C; spindle 14, 50 rpm
Optimal storage temperature 2–8 °C Store unopened in a dry location

After-processing / final-state properties

Typical properties of the heat-cured adhesive under the stated cure and test conditions.

Property Value Unit Method / condition
Shore hardness ≥70 Durometer D ISO 868; cured 30 minutes at 120°C
Glass transition temperature 56 °C ASTM E 228; cured 30 minutes at 125°C
Coefficient of thermal expansion, below Tg 62 × 10-6 K-1 ISO 11359-2; cured 30 minutes at 125°C
Coefficient of thermal expansion, above Tg 193 × 10-6 K-1 ISO 11359-2; cured 30 minutes at 125°C
Elongation at break 2.98 % ISO 527-3; cured 30 minutes at 125°C
Tensile strength 62 N/mm² ISO 527-3; cured 30 minutes at 125°C; 8,970 psi
Tensile modulus 2,383 N/mm² ISO 527-3; cured 30 minutes at 125°C; 345,500 psi
Lap shear strength ≥13.8 N/mm² Etched aluminum, 0.125 mm gap; cured 30 minutes at 120°C; ≥2,000 psi