LOCTITE EA 3943

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 3943

Main features

  • Cannula-Focused Medium-Viscosity Dispensing
  • Sub-5-Second UV Fixture
  • UV-Fluorescent Assembly Inspection

Product Description

LOCTITE AA 3943 is a one-part, medium-viscosity UV and visible-light acrylic adhesive for bonding stainless-steel cannulae into hubs, syringes and lancets. Its 6,000 to 7,500 mPa s viscosity at 25 deg C is suited to dispensing on cannulae before hub assembly, including larger-gap needle configurations. The adhesive fixtures in less than 5 seconds under the stated 365 nm UV conditions and fluoresces under black light for assembly inspection. The cured material combines 271% elongation at break with Shore D 69 hardness, supporting flexible medical-device bonds across the specified glass, plastic and metal substrates.

Key features

  • Needle-assembly viscosity: 6,000 to 7,500 mPa s at 25 deg C supports controlled cannula-to-hub dispensing.
  • Fast light cure: Fixture time is less than 5 seconds at 30 mW/cm^2 and 365 nm on glass.
  • Inspection fluorescence: UV fluorescence supports visual confirmation of adhesive presence in bonded assemblies.

Applications

Applications include stainless-steel cannula bonding in hubs, syringes and lancets, plus documented glass, plastic and metal component bonding for disposable medical-device assembly.

Product Family

LOCTITE EA 3943

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent to hazy liquid, Free of undissolved solids
Specific Gravity
1.04
Physical Properties
Viscosity
6,000 to 7,500 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
55 °C
Chemical Properties
Water Absorption
4.4 / 4.2 %
Mechanical Properties
Elongation
271 %

Additional Information

Technical properties

As-supplied properties

Typical uncured-product values at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
AppearanceTransparent to hazy liquidFree of undissolved solids
UV fluorescencePositiveInspection under UV light
Specific gravity1.04At 25 deg C
Gardner color3 or lessTypical limit
Viscosity6,000 to 7,500mPa sBrookfield RVT, spindle 4, 20 rpm, 25 deg C
Technical properties

Final-state properties

Typical cured-material values after 100 mW/cm^2 at 365 nm for 30 seconds per side using an electrodeless D bulb, unless otherwise stated.

Property Value Unit Method / condition
Glass transition temperature55deg CASTM E 228
Shore hardness69Durometer DISO 868
Elongation at break271%ISO 527-3
Tensile strength24N/mm^2ISO 527-3
Tensile modulus441N/mm^2ISO 527-3
UV depth of cureAt least 1.5mm100 mW/cm^2 at 365 nm for 10 seconds, electrodeless D bulb
Block shear strength9.7N/mm^2ISO 13445, polycarbonate to polycarbonate, 100 mW/cm^2 at 365 nm for 30 seconds