LOCTITE EA 3942

Main features

  • 900-1,600 mPa s Dispensing
  • Sub-5-Second UV Fixture
  • UV-Fluorescent Assembly Inspection

Product Description

LOCTITE AA 3942 is a one-part, medium-viscosity UV and visible-light acrylic adhesive for disposable medical-device assembly. It is specifically designed for bonding stainless-steel cannulae into hubs, syringes and lancets and also bonds the specified plastic, glass and metal substrates. The 900 to 1,600 mPa s viscosity at 25 deg C supports controlled needle-assembly dispensing, while fixture develops in less than 5 seconds under the stated 365 nm UV conditions. UV fluorescence supports adhesive-presence inspection, and the cured material reaches Shore D 76 with 29 N/mm^2 tensile strength under the stated cure.

Key features

  • Controlled needle dispensing: Typical viscosity is 900 to 1,600 mPa s at 25 deg C.
  • Fast UV fixture: Fixture develops in less than 5 seconds at 30 mW/cm^2 and 365 nm on glass.
  • UV inspection: Positive fluorescence supports adhesive-presence checks in bonded assemblies.

Applications

Applications include stainless-steel cannula bonding in hubs, syringes and lancets, plus documented plastic, glass and metal bonding for disposable medical-device assembly.

Product Family

LOCTITE EA 3942

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent to hazy liquid, free of undissolved solids
Specific Gravity
1.03
Physical Properties
Viscosity
900 - 1,600 mPa.s
Mechanical Properties
Elongation
15 %
Thermal Properties
Glass Transition Temperature (Tg)
55 °C
Chemical Properties
Water Absorption
5.0/4.8 %

Additional Information

Technical properties

As-supplied properties

Typical uncured-product values at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
AppearanceTransparent to hazy liquidFree of undissolved solids
UV fluorescencePositiveInspection under UV light
Specific gravity1.03At 25 deg C
Gardner color3 or lessTypical limit
Viscosity900 to 1,600mPa sBrookfield RVT, spindle 2, 20 rpm, 25 deg C
Technical properties

Final-state properties

Typical cured-material values after 100 mW/cm^2 at 365 nm for 30 seconds using an electrodeless D bulb, unless otherwise stated.

Property Value Unit Method / condition
Shore hardness76Durometer DISO 868
Linear shrinkage2.0%Cured material
Elongation at break15%ISO 527-3
Glass transition temperature55deg CASTM E 228
Tensile strength29N/mm^2ISO 527-3
Tensile modulus986N/mm^2ISO 527-3
UV depth of cureAt least 1.5mm100 mW/cm^2 at 365 nm for 10 seconds, electrodeless D bulb
Block shear strength11.1N/mm^2Polycarbonate to polycarbonate, 100 mW/cm^2 at 365 nm for 10 seconds