LOCTITE EA 11C

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

LOCTITE EA 11C

Main features

  • Machinable, Low-Outgassing Cured Material
  • Bonds Metals, Most Plastics and Wood
  • Room-Temperature or Heat Cure

Product Description

LOCTITE EA 11C is a black, two-part epoxy adhesive and sealant for general-purpose bonding, sealing, and repair of metals, most plastics, and wood. The resin and hardener mix at 100:38 by weight or 2.5:1 by volume and provide at least 20 minutes of pot life at 25 °C. The system cures at room temperature or with heat, reaches handling strength in approximately 3 to 4 hours at 25 °C, and develops full cure after 72 hours at 25 °C. Once cured, the material can be machined and sanded and has documented high-service-temperature and low-outgassing characteristics.

Key features

  • Multi-material bonding and repair for metals, most plastics, and wood.
  • Room-temperature or heat cure with at least 20 minutes of pot life at 25 °C.
  • Machinable, low-outgassing cured material with documented high-service-temperature capability.

Applications / Suitable for

  • General-purpose bonding, sealing, and repair of metals, most plastics, and wood.
Product Family

LOCTITE EA 11C

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black / Green
Component System
Two (Resin / Hardener)
Mix Ratio
100 : 38 by weight
Pot Life
≥20 minutes
Specific Gravity
1.6 / 1.67
Thermal Properties
Glass Transition Temperature (Tg)
114 °C
Thermal Conductivity
0.75 W/m.K
Electrical Properties
Dielectric Strength
18.5 kV/mm
Volume Resistivity
5.0×10¹⁴ Ohms⋅cm
Other Properties
Storage Temperature
8-21 °C

Leading Brands Trust in Our Products and Services