Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE E-40FL

Main features

  • Toughened Epoxy Bonding
  • Medium Owrking Life
  • Shock and Vibration Resistance

Product Description

LOCTITE® EA E-40FL™ is a toughened, medium-viscosity, two-component epoxy adhesive designed for flexible bonding applications requiring excellent shock and impact resistance. After mixing, the adhesive cures at room temperature to form a flexible gray bond line with strong adhesion to plastics, metals, glass, wood, ceramics, rubber and masonry. The cured material provides good chemical and solvent resistance together with excellent electrical insulation characteristics, making it suitable for bonding dissimilar materials and low-stress, high-impact assemblies.

Key Features & Benefits

  • Toughened two-component epoxy adhesive.
  • Flexible cured bond line with excellent impact resistance.
  • Medium working life for convenient assembly operations.
  • Excellent resistance to shock and vibration.
  • Good chemical and solvent resistance after cure.
  • Excellent electrical insulation properties.
  • Suitable for bonding dissimilar materials.

Recommended Applications

  • Plastic, metal, glass and ceramic bonding.
  • Rubber-to-metal bonding applications.
  • Repair of strain gauges and printed circuit boards.
  • Sealing fiberglass component seams.
  • Bonding stainless steel inserts and hose assemblies.
Product Family

LOCTITE E-40FL

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Gray, opaque liquid
Mix Ratio
1:1
Specific Gravity
1.3/1.1
Physical Properties
Viscosity
60,000 to 90,000/50,000 to 85,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Epoxy — Two-component adhesive
Appearance (Resin) Off-white to Beige Liquid — Part A
Appearance (Hardener) Dark Gray Liquid — Part B
Appearance (Mixed) Gray Opaque Liquid — Mixed adhesive
Mix Ratio (Volume) 1 : 1 Resin : Hardener By volume
Mix Ratio (Weight) 100 : 85 Resin : Hardener By weight
Resin Viscosity 60,000 - 90,000 mPa·s (cP) Brookfield RVT, 25°C
Hardener Viscosity 50,000 - 85,000 mPa·s (cP) Brookfield RVT, 25°C
Specific Gravity (Mixed) 1.2 — 25°C
Working Life 40 minutes 25°C
Tack Free Time 130 minutes Typical
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 30 °C Cured @ 25°C
Shore Hardness 75 Shore D ISO 868
Elongation 22 % ISO 527-2
Tensile Strength 16 N/mm² ISO 527-2
Dielectric Breakdown Strength 16 kV/mm IEC 60243-1
Lap Shear Strength (Aluminum) 25.9 N/mm² 3 days @ 22°C
Lap Shear Strength (Steel) 4.4 N/mm² Grit blasted steel
Block Shear Strength (Epoxy) 11 N/mm² ISO 13445
Block Shear Strength (Glass) 12.9 N/mm² ISO 13445
Accelerated Cure Strength ≥6.9 N/mm² 2 h @ 65°C, Aluminum