LOCTITE E-05MR

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE E-05MR

Main features

  • Ultra-Clear 1:1 Epoxy
  • Fast Adhesive Fixture
  • 34 kV/mm Dielectric Strength

Product Description

LOCTITE® EA E-05MR™ is a general-purpose, two-component epoxy adhesive that develops high bond strength on a wide range of substrates. The ultra-clear formulation cures at room temperature to form a water-white transparent bond line with excellent impact resistance and gap-filling capability. It is particularly suitable for bonding metals, ceramics, rigid plastics and wood where optical clarity and durable structural performance are required.

Key Features & Benefits

  • Ultra-clear, water-white cured bond line.
  • Two-component room-temperature curing epoxy.
  • Excellent impact resistance after cure.
  • Gap-filling capability for rough or poorly fitting surfaces.
  • High bond strength on multiple substrates.
  • Good electrical insulation properties.
  • Suitable for metal, ceramic, plastic and wood bonding.

Recommended Applications

  • General-purpose industrial bonding.
  • Clear structural adhesive assemblies.
  • Metal and ceramic bonding.
  • Rigid plastic assembly.
  • Wood bonding and repair.
Product Family

LOCTITE E-05MR

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Ultra clear
Mix Ratio
1:1
Specific Gravity
1.16
Physical Properties
Viscosity
18,000 - 25,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Epoxy — Two-component adhesive
Appearance (Resin) Ultra Clear — Part A
Appearance (Hardener) Ultra Clear — Part B
Appearance (Mixed) Water White Clear Liquid — Mixed adhesive
Mix Ratio 1 : 1 Resin : Hardener By volume and weight
Resin Viscosity 18,000 - 25,000 mPa·s (cP) 100 s⁻¹ shear rate
Hardener Viscosity 18,000 - 25,000 mPa·s (cP) 100 s⁻¹ shear rate
Specific Gravity (Mixed) 1.16 — 25°C
Gel Time 7 - 12 minutes 22°C
Fixture Time 10 - 15 minutes Steel, 22°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 39 °C ISO 11359-2
Shore Hardness 78 Shore D ISO 868
Elongation at Break 4.5 % ISO 527-3
Tensile Strength 50 N/mm² ISO 527-3
Tensile Modulus 1,500 N/mm² ISO 527-3
Dielectric Breakdown Strength 34 kV/mm IEC 60243-1
Lap Shear Strength (Steel) 23 N/mm² 5 days @ 22°C
Lap Shear Strength (Aluminum) 24 N/mm² 2 h @ 65°C cure
Impact Strength (Steel) 5 J ISO 9653
Impact Strength (Aluminum) 6 J ISO 9653

Leading Brands Trust in Our Products and Services