LOCTITE E-00CL

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE E-00CL

Main features

  • 1:1 Two-Component Epoxy
  • 3.5-Minute Working Life
  • Electrically Insulating Epoxy

Product Description

LOCTITE® EA E-00CL™ is a fast-setting, two-component clear epoxy adhesive formulated for general-purpose structural bonding, potting, and encapsulation applications. The adhesive cures at room temperature to form a clear, rigid, machinable bond line with excellent electrical insulation properties and resistance to a wide range of chemicals and solvents. It bonds effectively to metals, plastics, glass, ceramics, rubber, and wood, making it ideal for applications where a transparent bond line is required.

Key Features & Benefits

  • Two-component clear epoxy adhesive system.
  • Fast room-temperature cure after mixing.
  • Low-viscosity formulation for easy dispensing.
  • Clear, machinable cured bond line.
  • Excellent electrical insulating characteristics.
  • Good resistance to chemicals and solvents.
  • Bonds metals, plastics, glass, wood, ceramics and rubber.

Recommended Applications

  • General-purpose industrial bonding.
  • Potting and encapsulation.
  • Electrical insulation applications.
  • Transparent bond line assemblies.
  • Plastic, metal, glass and ceramic bonding.
Product Family

LOCTITE E-00CL

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear (mixture)
Mix Ratio
1:1
Specific Gravity
1.1
Physical Properties
Viscosity
7,000 - 13,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Epoxy — Two-component adhesive
Appearance (Resin) Clear to Slight Yellow — Liquid
Appearance (Hardener) Clear to Slight Yellow — Liquid
Mix Ratio (Volume) 1 : 1 Resin : Hardener By volume
Mix Ratio (Weight) 100 : 100 Resin : Hardener By weight
Resin Viscosity 7,000 - 13,000 mPa·s (cP) 25°C
Hardener Viscosity 2,200 - 4,500 mPa·s (cP) 25°C
Specific Gravity 1.1 — Resin, Hardener and Mixed
Working Life 3.5 minutes 25°C
Tack Free Time 4 minutes 25°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 20 °C Cured at 25°C
Shore Hardness 80 Shore D ISO 868
Elongation 13 % ISO 527-2
Tensile Strength 26 N/mm² ISO 527-2
Dielectric Breakdown Strength 16 kV/mm IEC 60243-1
Lap Shear Strength (Aluminum) ≥6.9 N/mm² ISO 4587, 2 h @ 65°C cure
Lap Shear Strength (Steel) 15 N/mm² 5 d @ 22°C cure
Lap Shear Strength (Stainless Steel) 13 N/mm² 5 d @ 22°C cure
Block Shear Strength (PVC) 17 N/mm² ISO 13445
Block Shear Strength (Glass) 15 N/mm² ISO 13445