LOCTITE ABP 2100ANP | PFAS-Free Die Attach Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABP 2100ANP

Main features

  • Formulated for Pb-free applications
  • High hot/wet adhesion
  • Excellent dispensability

Product Description

LOCTITE® ABLESTIK ABP 2100ANP is an electrically conductive die attach adhesive engineered for high-throughput, Pb-free Ball Grid Array (BGA) packaging. It's designed to withstand the high reflow temperatures (up to 260°C) required for Pb-free solders and meets automotive-grade standards. This adhesive is suitable for die sizes up to 12.7 mm x 12.7 mm and does not contain any intentionally added PFAS.

Recommended Cure Schedule

  • 30 minutes ramp to 175°C + 15 minutes @ 175°C in N2
  • 30 minutes ramp to 175°C + 30 minutes @ 175°C in N2

Product Key Features

  • Electrically conductive
  • High-temperature resistance — Withstands Pb-free reflow temperatures up to 260°C.
  • Automotive grade — Meets rigorous reliability standards for automotive applications.
  • PFAS-free — Does not contain intentionally added per- and polyfluoroalkyl substances.

Applications

Product Family

LOCTITE ABP2100ANP

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 33 days
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
3.1 g/cm3
Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
54 °C
Thermal Conductivity
1.2 W/m.K
Weight Loss @ 300°C
1.83 %
Chemical Properties
Moisture absorption
0.24 %
Physical Properties
Thixotropic index
5
Viscosity
11,750 mPa.s

Additional Information

Thawing

  1. Allow container to reach room temperature before use.
  2. After removing from the freezer, set the syringes to stand vertically while thawing.
  3. Thaw times depend on the syringe size.
  4. Consult handling guide for more information.
  5. DO NOT open the container before contents reach 25°C temperature. Any moisture that collects on the thawed container should be removed prior to opening the container.
  6. DO NOT re-freeze. Once thawed to 25°C, the adhesive should not be re-frozen.

ABP2100ANPThawCurve

Directions for Use

  1. Thawed material should immediately be placed on dispense equipment for use.
  2. If the adhesive is transferred to a final dispensing reservoir, care must be exercised to avoid entrapment of contaminants and/or air into the adhesive.
  3. Adhesive must be completely used within the product's recommended work life.
  4. Alternate dispense amounts may be used depending on the application requirements.
  5. Star or crossed shaped dispense patterns will yield fewer bondline voids than the matrix style of dispense pattern.