LOCTITE AA 3974

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE AA 3974

Main features

  • Rapid UV/Visible-Light Fixture
  • Thermal-Cycling-Resistant Cured Adhesive
  • Potting/Sealing/Bonding Assembly Applications

Product Description

LOCTITE® AA 3974™ is a one-component UV and visible light-curing acrylic adhesive designed for potting, sealing and bonding thermoplastics, glass and metals exposed to thermal cycling and environmental aging. The product offers rapid curing under UV or visible light, develops flexible and durable bond lines, and is suitable for disposable medical device assembly. It has been tested against ISO 10993-based biocompatibility protocols and is widely used where high-speed curing and reliable long-term performance are required.

Key Features & Benefits

  • One-component UV/visible light curing acrylic adhesive.
  • Rapid fixture times of approximately 5 seconds under LED systems.
  • Suitable for bonding thermoplastics, glass and metals.
  • Excellent resistance to thermal cycling and environmental exposure.
  • Designed for potting, sealing and bonding applications.
  • Suitable for disposable medical device assembly.
  • Tested to ISO 10993-based biocompatibility protocols.

Recommended Applications

  • Medical device assembly and disposable device manufacturing.
  • Glass, thermoplastic and metal bonding.
  • Potting electronic and industrial components.
  • High-speed UV-curable sealing operations.
  • Assemblies exposed to thermal cycling and environmental aging.
Product Family

LOCTITE AA 3974

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent colorless liquid
Specific Gravity
1.09
Physical Properties
Viscosity
2400 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology UV Acrylic — UV / Visible Light Cure
Appearance Translucent Colorless Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.09 — 25°C
Density 1.106 g/cm³ 20°C
Viscosity 2,400 mPa·s (cP) Cone & Plate, 25°C
Flash Point 81.5 °C Pensky-Martens Closed Cup
UV Fixture Time 5 seconds 100 mW/cm² @ 365 or 405 nm LED
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Shore Hardness 77 Shore A ISO 868
Tensile Strength 33 N/mm² ISO 527-3
Elongation at Break 100 % ISO 527-3
Linear Shrinkage 2.6 % ASTM D792
Water Absorption 5.8 % 2 h in boiling water, ISO 62
Surface Resistivity 1.25 × 10¹⁴ Ω IEC 60093
Volume Resistivity 1.1 × 10¹² Ω·cm IEC 60093
Dielectric Breakdown Strength 17 kV/mm IEC 60243-1
Dielectric Constant / Dissipation Factor 5.43 / 0.15 — 1 kHz, IEC 60250
Block Shear Strength (Polycarbonate to Polycarbonate) 13 N/mm² ISO 13445
Needle Pullout Strength 19 N Polycarbonate hub to stainless steel cannula
VOC Content 9.9 % SDS, Section 15