LOCTITE AA 3751

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

LOCTITE AA 3751

Main features

  • Solvent-Free 100% Solids
  • 10-Second UV Fixture
  • Multi-Function UV Processing

Product Description

LOCTITE AA 3751 is a one-part, solvent-free modified acrylic ester adhesive for UV-light tacking, bonding, coating, encapsulating and sealing. The transparent amber-to-yellow liquid is 100% non-volatile and has medium, shear-dependent Brookfield viscosity for controlled dispensing and coverage. Under the stated UV conditions, fixture develops in 10 seconds or less on glass slides. Cured films reach Shore D 73 hardness and 50% elongation at break. This combination supports assembly processes that use one UV-curing material for bonding, coating, encapsulation and sealing.

Key features

  • Solvent-free formulation: The one-part material is 100% solids with no mixing required.
  • Fast UV fixture: Fixture develops in 10 seconds or less on glass slides at 6 mW/cm^2 and 365 nm.
  • Multi-function application: One grade supports tacking, bonding, coating, encapsulating and sealing.

Applications

Applications include UV-light tacking, bonding, coating, encapsulating and sealing.

Product Family

LOCTITE AA 3751

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Modified acrylic ester
Color
Transparent amber to yellow liquid
Component System
One component
Solids
100 %
Physical Properties
Tack-Free Time
≤60 seconds minutes
Viscosity
8,000 to 15,000 mPa.s
Mechanical Properties
Elongation
50 %
Electrical Properties
Dielectric Strength
29 kV/mm
Surface Resistivity
1.3×10^16 Ohms/sq
Volume Resistivity
5.4×10^14 Ohms⋅cm
Physical Properties
Depth of Cure
3.5 mm

Additional Information

Technical properties

As-supplied properties

Typical uncured-product values at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
AppearanceTransparent amber to yellow liquidUncured
Solids / non-volatile content100%As supplied
Viscosity8,000 to 15,000mPa sBrookfield RVT, spindle 4, 2.5 rpm, 25 deg C
Viscosity3,600 to 7,000mPa sBrookfield RVT, spindle 4, 20 rpm, 25 deg C
Technical properties

Final-state properties

Typical cured-film values for 0.6 to 0.8 mm films cured at 30 mW/cm^2 and 365 nm for 2 minutes per side using a Zeta 7400 source, unless otherwise stated.

Property Value Unit Method / condition
Shore hardness73Durometer DISO 868
Elongation at break50%ISO 527-3
Tensile strength at yield22.7N/mm^2ISO 527-3
Tensile strength at break11N/mm^2ISO 527-3
Tensile modulus634N/mm^2ISO 527-3
UV depth of cure3.5mm25 mW/cm^2 at 365 nm for 10 seconds, Zeta 7400
Lap shear strength4.8N/mm^2ISO 4587, polycarbonate to polycarbonate; substrate failure