LOCTITE AA 3526

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE AA3526

Main features

  • Translucent
  • Cures rapidly
  • Excellent adhesion to glass, plastics and metals

Product Description

LOCTITE® AA 3526 is a translucent, pale straw to amber, 1-part, medium viscosity, UV/visible light-cured, liquid modified acrylic adhesive. It cures rapidly to form flexible, transparent bonds when exposed to ultraviolet light and/or visible light of sufficient irradiance. The secondary cure system permits cure of product in shadowed areas.

LOCTITE® AA 3526 is an Acrylic, monocomponent liquid with positive fluoresence under UV light. It's bonding cure profile benefits high speed curing production lines.

LOCTITE® AA 3526 can be cured by exposure to UV and/or visible light radiation or heat . The speed and depth of cure will depend on the UV intensity measured at the product surface.

Heat Cure

  • 15minutes at 121°C

Fixture Time

Fixture time is defined as the time to develop a shear strength of 0.1 N/mm².

UV Fixture Time, Glass microscope slides, seconds:

  • Black light, Zeta® 7500 light source:
  • 6 mW/cm², measured @ 365 nm ≤5LMS
Product Family

LOCTITE AA 3526

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 15 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Refractive index
1.51
Specific Gravity
1.06
Thermal Properties
Glass Transition Temperature (Tg)
36 °C
Mechanical Properties
Elongation
185 %
Chemical Properties
Water Absorption
5.6 %
Physical Properties
Viscosity
17,500 mPa.s