Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE AA 3525

Main features

  • Rapid Cure Speed
  • Clear, Colorless Bondline
  • Good Moisture and Humidity Resistance

Product Description

LOCTITE® AA 3525™ is a one-component, UV/visible light-curing modified acrylic adhesive developed for high-speed bonding applications requiring clear, durable and flexible bond lines. The product rapidly cures upon exposure to ultraviolet or visible light, forming transparent bonds with excellent toughness, flexibility and resistance to moisture exposure. It is designed for bonding glass, metals and plastics in industrial assembly operations and is also used in electric motor balancing applications where fast curing and reliable long-term performance are essential.

Key Features & Benefits

  • UV and visible light-curing modified acrylic adhesive.
  • Rapid cure speed for high-volume manufacturing.
  • Forms clear, colorless bond lines after curing.
  • Excellent flexibility, toughness and impact resistance.
  • Good moisture and humidity resistance.
  • One-component system requiring no mixing.
  • Suitable for glass, metal and plastic bonding applications.

Recommended Applications

  • Glass-to-glass and glass-to-metal bonding.
  • Industrial plastic and metal assembly.
  • Electric motor balancing operations.
  • Optically clear bonding applications.
  • High-speed production environments requiring instant curing.
Product Family

LOCTITE AA 3525

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent liquid
Specific Gravity
1.08
Physical Properties
Viscosity
15250 mPa.s