LOCTITE AA 352

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE AA 352

Main features

  • One-Component Adhesive System
  • Rapid UV Bonding Cure
  • Impact-Resistant Acrylic Bonding

Product Description

LOCTITE® AA 352™ is a one-component, UV-curable modified acrylic adhesive designed for high-speed bonding, coating and sealing applications. The product rapidly cures when exposed to ultraviolet light and can also be cured using heat or activator systems when required. Once cured, it offers excellent resistance to vibration, impact, humidity and environmental aging. LOCTITE AA 352 is commonly used for bonding glass and metal components, electrical devices, appliance parts and decorative assemblies where optical clarity, fast cure speed and durable performance are critical.

Key Features & Benefits

  • One-component UV-curable modified acrylic adhesive.
  • Rapid curing under UV light for high-speed production.
  • Secondary cure options by heat or activator.
  • Excellent resistance to vibration and impact loads.
  • Transparent cured appearance suitable for glass assemblies.
  • Suitable for bonding, sealing and coating applications.
  • Good environmental and humidity resistance after cure.

Recommended Applications

  • Glass-to-metal bonding.
  • Electrical device assembly and unitizing.
  • Appliance component bonding.
  • Decorative glass and metal assemblies.
  • Industrial sealing and coating operations.
Product Family

LOCTITE AA 352

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent light amber liquid
Refractive index
1.48
Specific Gravity
1.06
Physical Properties
Viscosity
20,500 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Modified Acrylic — UV-curable adhesive
Appearance Transparent Light Amber Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.06 — 25°C
Density 1.05 g/cm³ 20°C
Refractive Index 1.48 — ASTM D542
Viscosity 20,500 mPa·s (cP) Brookfield RVT, Spindle 6, 20 rpm, 25°C
UV Fixture Time 5 - 12 seconds 365 nm UV exposure
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 45 °C ISO 11357-2
Shore Hardness 60 Shore D ISO 868
Tensile Strength 24.4 N/mm² ISO 527-3
Elongation at Break 290 % ISO 527-3
Tensile Modulus 255 N/mm² ISO 527-2
Water Absorption 8.7 % Cured material
Volume Resistivity 8 × 10¹² Ω·cm IEC 60093
Dielectric Breakdown Strength 25 kV/mm IEC 60243-1
Dielectric Constant / Dissipation Factor 5.2 / 0.03 — 1 kHz, IEC 60250
Block Shear Strength (Steel to Glass) 16.5 N/mm² ISO 13445
Lap Shear Strength (Steel to Glass) 20.6 N/mm² Heat cured at 121°C
VOC Content <3.0 % 2010/75/EC