LOCTITE AA 3494

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE AA 3494

Main features

  • UV/Visible-Light Adhesive Cure
  • 10-Second or Faster Fixture
  • Electrically Insulating Acrylic Adhesive

Product Description

LOCTITE® AA 3494™ is a one-component, UV and visible light curing modified acrylic adhesive designed for bonding, sealing and potting applications. The transparent adhesive cures within seconds upon exposure to suitable ultraviolet light, producing tough, impact-resistant bonds with excellent resistance to humidity, water immersion and environmental aging. It is particularly well suited for glass bonding applications, including decorative glass assemblies, molded glass products and automotive lighting components where optical clarity and rapid production throughput are required.

Key Features & Benefits

  • UV and visible light curing acrylic adhesive.
  • Fast fixture and cure speeds for high-volume production.
  • Excellent adhesion to glass and dissimilar substrates.
  • Transparent cured appearance with refractive index close to glass.
  • High resistance to humidity, water immersion and environmental exposure.
  • Suitable for bonding, sealing and potting applications.
  • One-component formulation requiring no mixing.

Recommended Applications

  • Glass-to-glass bonding assemblies.
  • Decorative and molded glass products.
  • Automotive lighting component assembly.
  • Glass-to-metal and glass-to-plastic bonding.
  • UV-curable sealing and potting applications.
Product Family

LOCTITE AA 3494

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent liquid
Refractive index
1.48
Specific Gravity
1.02
Physical Properties
Viscosity
5000 - 7000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Modified Acrylic — UV / Visible Light Cure
Appearance Transparent Liquid — Uncured
Components One Part — No Mixing Required
Specific Gravity 1.02 — 25°C
Density 1.024 g/cm³ 20°C
Refractive Index 1.48 — Uncured Material
Viscosity 5,000 - 7,000 mPa·s Brookfield RVT, 25°C
Fixture Time ≤10 seconds 365 nm UV, 6 mW/cm²
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 31 °C ISO 11357-2
Shore Hardness 65 Shore D ISO 868
Tensile Strength 22.5 N/mm² ISO 527-3
Tensile Modulus 520 N/mm² ISO 527-3
Water Absorption 4.08 % 2 h Boiling Water, ISO 62
Volume Resistivity 3.3 × 10¹⁵ Ω·cm IEC 60093
Surface Resistivity 3.0 × 10¹⁵ Ω IEC 60093
Dielectric Breakdown Strength 32.3 kV/mm IEC 60250
Block Shear Strength (Steel to Glass) 16.8 N/mm² ISO 13445
VOC Content <5.0 % 2010/75/EC