LOCTITE AA 3412

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE AA 3412

Main features

  • High-Strength Structural Bonding
  • Non-Sag Placement Control
  • Fast Room Temperature Curing

Product Description

LOCTITE® AA 3412™ is a two-component, room-temperature-curing structural acrylic adhesive designed for high-strength bonding of metals, many plastics, composites, ceramics, fiberglass, and other rigid substrates. Its non-sag gel consistency supports vertical application and large-gap filling, while the mixed adhesive develops tough, impact-resistant, peel-resistant bonds with strong resistance to fuels, lubricants, cleaners, heat, humidity, and demanding industrial environments.

Key features

  • High-strength structural bonding: Delivers strong lap-shear, peel, and impact performance across metals, plastics, composites, and ceramics.
  • Non-sag gap filling: High-viscosity gel consistency supports vertical dispensing and bonding where larger gaps must be filled.
  • Fast room-temperature processing: Provides approximately five minutes of working time and fixtures on steel in about 12 to 15 minutes.
Product Family

LOCTITE AA 3412

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
White creamy soft gel/Amber gel
Mix Ratio
1:1
Specific Gravity
1.0
Physical Properties
Viscosity
150,000 - 450,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-material properties; processing performance depends on accurate proportioning, complete mixing, substrate preparation, application speed, bond geometry, and ambient temperature.

Property Value Unit Method / condition
Technology Acrylic — Structural adhesive technology
Chemical type — resin Methacrylate — Component A / resin
Chemical type — hardener Methacrylate — Component B / hardener
Resin appearance White to off-white creamy soft gel — TDS and Component A SDS
Hardener appearance Amber gel — TDS and Component B SDS
Mixed appearance Pale yellow-green opaque gel — After complete 1:1 mixing
Components Two components — Requires mixing before application
Mix ratio by weight 1:1 Resin:hardener TDS specified ratio
Mix ratio by volume 1:1 Resin:hardener TDS specified ratio
Cure mechanism Room-temperature cure after mixing — Two-component reaction cure
Resin specific gravity 1.00 — At 25°C; TDS
Hardener specific gravity 0.97 — At 25°C; TDS
Mixed specific gravity 0.99 — At 25°C
Resin viscosity 150,000–450,000 mPa·s Brookfield DVE, 25°C, spindle TD, 2.5 rpm, Helipath
Hardener viscosity 150,000–450,000 mPa·s Brookfield DVE, 25°C, spindle TD, 2.5 rpm, Helipath
Working time 5 min Mixed adhesive at 25°C
Fixture time 12–15 min ISO 4587, steel; time to reach 0.1 N/mm² shear strength
Component A flash point 10.6 °C Tagliabue closed cup; SDS
Component B flash point 10.6 °C Tagliabue closed cup; SDS