LOCTITE AA 3381

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE AA 3381

Main features

  • Fast 365 nm Light Fixturing
  • High-Elongation Glass Joint Sealing
  • Dissimilar Rigid-Substrate Bonding

Product Description

LOCTITE AA 3381 is a one-component, medium-viscosity acrylated urethane adhesive for UV-light bonding, potting, and sealing. The translucent colorless liquid requires no mixing and is intended primarily for glass-to-metal joints exposed to thermal cycling and environmental conditions. It also bonds dissimilar rigid substrates and reaches fixture strength in 15 seconds or less under the specified 365 nm light conditions. The cured material combines Shore A hardness of at least 72 with 330% elongation. Block-shear performance is characterized for glass-to-glass, glass-to-steel, glass-to-aluminum, and polycarbonate assemblies. Applications include disposable medical-device assembly.

Key features

  • Glass-to-Metal Joint Sealing: The product is intended for potting and sealing glass-to-metal joints exposed to thermal cycling and environmental conditions.
  • High-Elongation Cure: The cured material provides 330% elongation with Shore A hardness of at least 72.
  • Fast 365 nm Fixture: Fixture strength develops in 15 seconds or less under the listed 365 nm light conditions.

Applications / Suitable for

  • Potting and sealing glass-to-metal joints
  • Bonding dissimilar rigid substrates
  • Disposable medical-device assembly
Product Family

LOCTITE AA 3381

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Acrylated urethane
Component System
One component
Specific Gravity
1.08
Physical Properties
Viscosity
3,600 to 6,600 mPa.s
Chemical Properties
Water Absorption
4.9 %
Mechanical Properties
Elongation
330 %
Electrical Properties
Dielectric Strength
37 kV/mm
Volume Resistivity
1.06×10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTranslucent colorless-Uncured
Specific gravity1.08-25 deg C
Viscosity3,600 to 6,600mPa sBrookfield RVT, spindle 4, 20 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Shore hardness>=72Durometer AISO 868; cured 30 seconds at 100 mW/cm^2 and 365 nm, D bulb
Elongation at break330%ISO 527-3; same cure
Tensile strength at break7.91N/mm^2ISO 527-3; same cure
Tensile modulus18.6N/mm^2ISO 527-3; same cure
Dielectric breakdown strength37kV/mmIEC 60243-1; same cure
Block shear strength4.2N/mm^2ISO 13445; glass to glass; 0.127 mm gap; same cure
Block shear strength3.5N/mm^2ISO 13445; glass to steel; 0.127 mm gap; same cure