LOCTITE AA 3106

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE AA 3106

Main features

  • Transparent liquid
  • UV & Visible light cure
  • Enhances shock absorption

Product Description

LOCTITE® AA 3106 is a transparent acrylic liquid, primarily designed for bonding rigid or flexible PVC to polycarbonate where large gap filling capabilities and flexible joints are desired. The product has shown excellent adhesion to a wide variety of substrates including glass, many plastics and most metals. The thixotropic nature of LOCTITE® AA 3106TM reduces the migration of liquid product after application to the substrate.

LOCTITE® AA 3106 can be cured by exposure to UV and/or visible light of sufficient intensity. To obtain full cure on surfaces exposed to air, radiation @ 220 to 260 nm is also required. The speed of cure will depend upon the UV intensity and spectral distribution of the light source, the exposure time and the light transmittance of the substrates.

Product Family

LOCTITE AA 3106

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 75 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Refractive index
1.48
Specific Gravity
1.08
Electrical Properties
Volume Resistivity
770000000000000 Ohms⋅cm
Physical Properties
Viscosity
5,000 mPa.s
Mechanical Properties
Elongation
250 %

Additional Information

LOCTITE® AA 3106™ can be cured by exposure to UV and/or visible light of sufficient intensity. To obtain full cure on surfaces exposed to air, radiation @ 220 to 260 nm is also required. The speed of cure will depend upon the UV intensity and spectral distribution of the light source, the exposure time and the light transmittance of the substrates.