LOCTITE AA 3103

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 3103

Main features

  • UV/Visible-Light Adhesive Cure
  • High-Adhesion Adhesive Bonding
  • Polycarbonate Bonding Application

Product Description

LOCTITE® AA 3103™ is a one-component UV and visible light-curing acrylic adhesive specifically formulated for bonding polycarbonate components while minimizing the risk of stress cracking under typical molded stress conditions. The transparent, flexible adhesive cures rapidly upon exposure to suitable ultraviolet or visible light sources, enabling high-speed production processes. LOCTITE AA 3103 develops strong, transparent bonds with a wide variety of substrates including polycarbonate, glass, many plastics and most metals. Its thixotropic consistency reduces adhesive migration after application, allowing precise placement and improved bond-line control.

Key Features & Benefits

  • UV and visible light-curing adhesive for rapid processing.
  • Specially designed for bonding polycarbonate without stress cracking.
  • Forms flexible, transparent bonds.
  • Excellent adhesion to glass, plastics and metals.
  • Thixotropic formulation minimizes adhesive migration.
  • One-component system requiring no mixing.
  • Enhances load-bearing and shock-absorbing characteristics of bonded assemblies.

Recommended Applications

  • Polycarbonate-to-polycarbonate bonding.
  • Transparent plastic assembly applications.
  • Glass-to-plastic bonding.
  • Medical, electronic and industrial component assembly.
  • High-speed production environments utilizing UV curing systems.
Product Family

LOCTITE AA 3103

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent to slightly hazy liquid
Refractive index
1.48
Specific Gravity
1.13
Physical Properties
Viscosity
8,000 - 14,500 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — UV / Visible Light Cure
Chemical Type Acrylated Urethane — One-component adhesive
Appearance Transparent to Slightly Hazy — Liquid
Viscosity Classification Medium, Thixotropic — Uncured material
Specific Gravity 1.13 — 25°C
Refractive Index 1.48 — Uncured
Brookfield Viscosity 8,000 - 14,500 mPa·s RVT, spindle 5, 20 rpm, 25°C
Fixture Time ≤18 seconds UV cure, glass microscope slides
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Shore Hardness 51 Shore D ISO 868
Refractive Index 1.50 — Cured adhesive
Elongation at Break 260 % ISO 527-3
Tensile Strength at Break 17 N/mm² ISO 527-3
Tensile Modulus 207 N/mm² ISO 527-3
Lap Shear Strength 11 N/mm² ISO 4587, polycarbonate
Surface Resistivity 8.7 × 10¹⁴ Ω IEC 60093
Volume Resistivity 8.9 × 10¹⁴ Ω·cm IEC 60093
Dielectric Breakdown Strength 24 kV/mm IEC 60243-1

Leading Brands Trust in Our Products and Services