LOCTITE 962T

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 962T

Main features

  • Thixotropic Application Control
  • High-Strength Joint Sealing
  • Heat-Resistant Sealing Service

Product Description

LOCTITE® 962T™ is a one-component, high-strength anaerobic sealant designed for sealing and securing close-fitting cylindrical metal assemblies where resistance to product migration is important. The thixotropic red methacrylate ester liquid cures when confined between mating metal surfaces in the absence of air. Typical applications include engine block cup and core plugs, water-pump seals, hub-and-shaft assemblies, and other high-strength metal sealing applications.

Key features

  • Thixotropic non-migrating application: Helps limit movement of the liquid sealant after it is applied to the substrate.
  • High-strength cylindrical sealing: Seals and secures closely fitted metal plugs, shafts, hubs, and related assemblies.
  • Heat-resistant cured performance: Delivers 13.8 N/mm² compressive shear strength in the reported hot-strength and heat-aging tests.
Product Family

LOCTITE 962T

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Opaque red liquid
Specific Gravity
1.05
Physical Properties
Viscosity
4,000 - 13,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Opaque red liquid — TDS description; SDS confirms red liquid
Fluorescence Positive under UV light — Inspection aid
Components One component — No mixing required
Rheology Thixotropic — Designed to reduce migration after application
Cure mechanism Anaerobic — Cures when confined between closely fitted metal surfaces without air
Secondary cure Activator — TDS states approximately 2-hour cure on activated parts
Application Sealing — Cylindrical metal assemblies and core plugs
Strength classification High — Sealing and securing application
Specific gravity 1.05 — At 27°C; TDS value
Dynamic viscosity 4,000–13,000 mPa·s Brookfield RVT, 25°C; spindle 3, 2.5 rpm
Dynamic viscosity 1,400–3,500 mPa·s Brookfield RVT, 25°C; spindle 3, 20 rpm
Fixture time 30 min Time to develop 0.1 N/mm² shear strength
Density 1.05 g/cm³ At 25°C; SDS value
Flash point >100 °C Tagliabue closed cup; SDS value
Auto-ignition temperature >300 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on substrate, fit, activator use, cure time, surface preparation, temperature, and test method.

Property Value Unit Method / condition
Hot compressive shear strength 13.8 N/mm² ISO 10123; steel pins and collars; cured 1 week at 22°C and tested at 88°C
Compressive shear strength after heat aging 13.8 N/mm² ISO 10123; steel pins and collars; heat-aged 120 hours at 121°C and tested at 22°C
Cure time on activated parts 2 h TDS application guidance
Cure time on unactivated parts 24 h TDS application guidance

Leading Brands Trust in Our Products and Services