Loctite Ablestik 83C Conductive Epoxy Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 83C Conductive Epoxy Adhesive

Main features

  • Silver-Filled Epoxy Adhesive
  • 0.0004 ohm-cm Volume Resistivity
  • Electrical-Connection Epoxy Bonding

Product Description

LOCTITE® ABLESTIK 83C is a silver-filled, electrically conductive epoxy adhesive resin supplied as a smooth, thixotropic paste. Used with Catalyst 9 or Catalyst B 97, it forms conductive bonded connections to documented substrates including metals, glass, ceramics, and plastics. The adhesive is intended for electrical connections where hot soldering is impractical and for connections to conductive plastics that cannot be exposed to high temperatures. Catalyst selection provides either a general-purpose system with a shorter working life or a heat-cured system with a longer working life and higher documented use temperature.

Key features

  • Electrically conductive epoxy: Silver-filled formulation develops a typical cured volume resistivity of 0.0004 ohm-cm with either documented curing agent.
  • Thermally conductive bondline: Typical cured thermal conductivity is 2.6 W/m·K when prepared with Catalyst 9 or Catalyst B 97.
  • Two curing-agent options: Catalyst 9 provides a 45-minute working life at 25°C, while Catalyst B 97 provides a 24-hour working life and a higher documented use-temperature range.

Applications / Suitable for

  • Electrical connections where hot soldering is impractical
  • Electrical connections to conductive plastics that cannot be subjected to high temperatures
  • Bonding documented metal, glass, ceramic, and plastic substrates where electrical conductivity is required
Product Family

LOCTITE 83C

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Thixotropic Paste
Chemistry Type
Epoxy
Color
Silver

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties. Mixed-system values depend on the curing agent and specified mix ratio.

Property Value Unit Method or condition
Chemical type Epoxy — ABLESTIK 83C resin as supplied
Appearance Silver, thixotropic paste — Visual; resin as supplied
Density 3.00 g/cm³ TP-13; resin as supplied
Curing-agent viscosity Catalyst 9: 0.080–0.105
Catalyst B 97: 4–8
Pa·s Equivalent source values: 80–105 cP and 4,000–8,000 cP
Mix ratio Catalyst 9: 3.5
Catalyst B 97: 1.0
parts by weight Amount of curing agent per 100 parts of ABLESTIK 83C resin
Working life Catalyst 9: 45 minutes
Catalyst B 97: 24 hours
— ERF 13-70; 100 g mixed material at 25°C
Mixed density Catalyst 9: 2.81
Catalyst B 97: 2.95
g/cm³ TP-13; mixed system
Technical properties

After-processing / final-state properties

Typical cured properties. Values depend on the selected curing agent and documented cure schedule.

Property Value Unit Method or condition
Tensile lap-shear strength Catalyst 9: 6.8
Catalyst B 97: 9.6
MPa TP-21; aluminum-to-aluminum; tested at 25°C; source equivalents 1,000 psi and 1,400 psi
Coefficient of thermal expansion 45 10−6/°C TMA; Catalyst 9 and Catalyst B 97 systems
Thermal conductivity 2.6 W/m·K ASTM D2214; Catalyst 9 and Catalyst B 97 systems; source equivalent 18 Btu-in/hr-ft²-°F
Temperature range of use Catalyst 9: −40 to +130
Catalyst B 97: −55 to +155
°C Documented range by curing-agent system
Volume resistivity at 25°C 0.0004 ohm-cm TP-296; Catalyst 9 and Catalyst B 97 systems
Total mass loss 0.64 % NASA outgassing; sample cured 1 hour at 66°C; curing-agent system not identified
Collected volatile condensable material 0.02 % NASA outgassing; sample cured 1 hour at 66°C; curing-agent system not identified