LOCTITE 736

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 736

Main features

  • Passive-Surface Cure Acceleration
  • Very-Low-Viscosity Surface Wetting
  • 30-Minute On-Part Activity

Product Description

LOCTITE SF 736 is a light-amber, very-low-viscosity activator for accelerating cure of anaerobic structural adhesives and sealants. The aldehyde-amine condensate and organocopper active system is carried in trichloroethylene and isopropanol. It is applied to passive metals, inert surfaces, or assemblies with larger gaps where the anaerobic process needs activation. A viscosity of 3 mPa s supports rapid surface wetting. The treated surface remains active for up to 30 minutes, allowing adhesive application within a defined process window.

Key features

  • Passive-surface cure acceleration: The activator supports anaerobic adhesive and sealant cure on passive metals and inert surfaces.
  • Very-low-viscosity wetting: A viscosity of 3 mPa s supports rapid application over prepared surfaces.
  • 30-minute on-part activity: The treated surface remains active for up to 30 minutes under the listed condition.

Applications / Suitable for

  • Activating passive metal surfaces
  • Accelerating anaerobic structural adhesives
  • Accelerating anaerobic sealants or larger-gap assemblies
Product Family

LOCTITE 736

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Light amber liquid
Chemistry Type
Aldehyde-amine condensate and Organocopper compound
Specific Gravity
1.3
Physical Properties
Viscosity
1 mPa.s
General Properties
Solvent
Trichlorethylene and Isopropanol

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceLight amber liquid-As supplied
Active systemAldehyde-amine condensate and organocopper-As supplied
SolventsTrichloroethylene and isopropanol-Carrier system
Specific gravity1.3-25 deg C
Viscosity3mPa s20 deg C
On-part life<=30minAfter application