LOCTITE 713

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 713

Main features

  • Pre- or Post-Applied Activation
  • Rapid 30-Second Drying
  • Short Controlled On-Part Window

Product Description

LOCTITE SF 713 is a transparent, colorless to slightly amber, very-low-viscosity cyanoacrylate activator for pre- or post-application cure acceleration. The amine active ingredient is supplied in isopropanol and dries in 30 seconds or less at 20 deg C. Its short on-part life of one minute or less supports rapid, controlled assembly sequences rather than long staging intervals. The activator is used with compatible cyanoacrylate adhesives to secure wires or coils to printed circuit boards, tamperproof adjustable components, and mount stand-offs, edge guides, or board stiffeners.

Key features

  • Pre- or post-application use: The activator can be applied before adhesive placement or to exposed adhesive afterward.
  • Rapid 30-second drying: The isopropanol carrier dries in 30 seconds or less at 20 deg C.
  • Short controlled process window: On-part activity lasts one minute or less under the listed condition.

Applications / Suitable for

  • Securing wires and coils to printed circuit boards
  • Tamperproofing adjustable components
  • Mounting stand-offs, edge guides, and board stiffeners
Product Family

LOCTITE 713

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent colorless to slightly amber liquid
Chemistry Type
Amine (active ingredient)
Specific Gravity
0.8
Physical Properties
Viscosity
1 mPa.s
Physical Properties
Drying Time
≤30 seconds
General Properties
Solvent
Isopropanol

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to slightly amber liquid-As supplied
Active ingredientAmine-1.7% to 2.3%
SolventIsopropanol-Carrier
Specific gravity0.8-25 deg C
Viscosity1mPa s20 deg C
Drying time<=30s20 deg C
On-part life<=1minAfter application