LOCTITE 641

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 641 LOCTITE 641 LOCTITE 641 LOCTITE 641

Main features

  • Serviceable Medium-Strength Retention
  • Controlled Medium-Viscosity Flow
  • Anaerobic One-Part Metal Cure

Product Description

LOCTITE 641 is a yellow, medium-viscosity one-component anaerobic retaining compound for cylindrical metal parts that may require later service disassembly. It cures between close-fitting metal surfaces after air is excluded and is commonly used to retain bearings on shafts or in housings. The shear-thinning viscosity profile supports controlled coverage during assembly. After 24 hours at 22 deg C, the cured compound develops at least 6.5 N/mm^2 compressive-shear strength on steel pins and collars. Medium-strength retention balances secure positioning with removal using appropriate service methods.

Key features

  • Serviceable medium-strength retention: The cured joint retains cylindrical parts while supporting later disassembly with appropriate methods.
  • Controlled medium-viscosity flow: Brookfield viscosity data support coverage without excessive run-off during assembly.
  • Anaerobic one-part processing: The compound cures in confined metal fits without mixing.

Applications / Suitable for

  • Retaining bearings on shafts
  • Retaining bearings in housings
  • Bonding cylindrical metal parts requiring service disassembly
Product Family

LOCTITE 641

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methacrylate ester
Color
Yellow liquid
Component System
One component
Specific Gravity
1.07
Thermal Properties
Linear thermal expansion
80×10^-6 K -1
Specific Heat Capacity
0.3 J/(g⋅°C)
Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity
400 to 800 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceYellow liquid-As supplied
Chemical typeMethacrylate ester-One-component material
Specific gravity1.07-25 deg C
Viscosity1,215 to 2,750mPa sBrookfield RVT, spindle 2, 2.5 rpm, 25 deg C
Viscosity400 to 800mPa sBrookfield RVT, spindle 2, 20 rpm, 25 deg C
Viscosity90 to 180mPa sEN 12092-MV, 277 s^-1, 25 deg C
Cure mechanismAnaerobic-Confined between close-fitting metal surfaces
Technical properties

After-processing / final-state properties

Typical values for the cured, bonded, treated, or in-service product under the listed conditions.

PropertyValueUnitMethod / condition
Compressive shear strength>=6.5N/mm^2Steel pins and collars, cured 24 h at 22 deg C
Coefficient of thermal expansion80 x 10^-6K^-1Cured material
Thermal conductivity0.1W/(m K)Cured material
Specific heat0.3kJ/(kg K)Cured material