Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 566

Main features

  • Low-Strength Thread Sealing
  • Vibration-Resistant Thread Sealing
  • One-Component Sealing System

Product Description

LOCTITE® 566™ is a one-component, low-strength anaerobic thread sealant designed for locking and sealing close-fitting metal pipes and fittings. The brown dimethacrylate ester liquid cures when confined between mating metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. It is formulated to seal against water, oil, and most common organic materials while supporting later disassembly with standard hand tools.

Key features

  • Low-strength thread sealing: Seals metal pipes and fittings while supporting service disassembly.
  • Vibration-resistant locking: Helps prevent loosening and leakage caused by shock and vibration.
  • One-component anaerobic cure: Requires no mixing and cures when confined between close-fitting metal surfaces.
Product Family

LOCTITE 566

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Brown liquid
Specific Gravity
1.05
Physical Properties
Viscosity
800 - 1,600 mPa.s
Thermal Properties
Thermal Conductivity
0.1 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Dimethacrylate ester — Uncured material
Appearance Brown liquid — Uncured material
Components One component — No mixing required
Strength classification Low — Thread-sealing application
Specific gravity 1.05 — At 25°C
Viscosity 800–1,600 mPa·s Brookfield LVF, 25°C; spindle 2, 20 rpm
Viscosity 300–400 mPa·s Brookfield LVF, 25°C; spindle 2, 30 rpm
Density 1.05 g/cm³ At 20°C; SDS value
Flash point >100 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, bond gap, temperature, activator use, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 100 × 10−6 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured-material property
Breakaway specific resistance 2–5 N·m M10 steel nuts and bolts; cured 24 hours at 22°C
Prevail specific resistance 1.6–4 N·m M10 steel nuts and bolts; cured 24 hours at 22°C
Breakaway torque 6–12 N·m ISO 10964; M10 steel nuts and bolts; cured 24 hours at 22°C
Prevail torque 5–11 N·m ISO 10964; M10 steel nuts and bolts; cured 24 hours at 22°C
Motor-oil resistance 100 % initial strength 5W/30 motor oil at 125°C; 1,000-hour exposure
Water/glycol resistance 90 % initial strength 50/50 water/glycol at 87°C; 1,000-hour exposure
Acetone resistance 80 % initial strength At 22°C; 1,000-hour exposure

Leading Brands Trust in Our Products and Services