LOCTITE 554

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 554

Main features

  • High Solvent Resistance
  • Thread Sealing Up to 50mm
  • One-Component Sealing System

Product Description

LOCTITE® 554 is a one-component, medium-viscosity anaerobic thread sealant formulated for metal threaded fittings and pipe up to 50 mm in diameter. The red methacrylate ester liquid cures when confined between close-fitting metal surfaces in the absence of air, providing maximum solvent resistance in demanding service environments. It is recommended for refrigeration systems and applications involving strong chemicals, including metal and fiber plants, chemical and paper processing facilities, waste treatment operations, and textile manufacturing.

Key features

  • High solvent resistance: Designed for threaded fittings exposed to refrigeration service and strong chemicals.
  • Thread sealing up to 50 mm: Intended for close-fitting metal pipe and fittings up to 2 inches in diameter.
  • One-component anaerobic cure: Requires no mixing and cures when confined between mating metal surfaces.
Product Family

LOCTITE 554

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red liquid
Specific Gravity
1.02
Physical Properties
Viscosity
1,500 - 3,500 mPa.s
Thermal Properties
Thermal Conductivity
0.1 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Red liquid — Uncured material
Fluorescence Negative — Uncured material
Components One component — No mixing required
Specific gravity 1.02 — At 25°C
Viscosity 1,500–3,500 mPa·s Brookfield RVT, 25°C; spindle 3, 20 rpm
Flash point >100 °C SDS value
Density 1.08 g/cm³ At 20°C; SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, specimen, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 0.1 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured-material property
Prevail torque ≥10.8 N·m ISO 10964; 3/8 × 24 steel nuts and bolts; cured 24 hours at 22°C
Breakaway torque 27.2 N·m ISO 10964; 3/8 × 24 steel nuts and bolts; cured 72 hours at 22°C
Prevail torque 23.8 N·m ISO 10964; 3/8 × 24 steel nuts and bolts; cured 72 hours at 22°C
Maximum application temperature 149 °C Typical stated application limit