LOCTITE 542

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE 542 LOCTITE 542

Main features

  • Low-Viscosity Fine-Thread Sealing
  • Anaerobic One-Part Application
  • Medium-Strength Serviceable Retention

Product Description

LOCTITE 542 is a brown, low-viscosity one-component anaerobic thread sealant for locking and sealing metal pipes and fittings. The thixotropic liquid remains controlled during application and cures between close-fitting metal threads in the absence of air. Medium-strength retention supports secure assemblies while allowing service with appropriate tools. Properly tightened fittings can seal immediately to moderate pressure, while at least 24 hours is recommended before maximum pressure or solvent resistance is required. The product is suited to fine-threaded metal fittings where a liquid sealant and controlled flow are needed.

Key features

  • Low-viscosity thread wetting: A 400 to 800 mPa s Brookfield range supports penetration and coverage on fine metal threads.
  • Anaerobic metal-thread cure: The one-part sealant cures between close-fitting metal surfaces without mixing.
  • Medium-strength service retention: Measured torque values support locking with later disassembly using appropriate tools.

Applications / Suitable for

  • Locking and sealing metal pipes
  • Fine-threaded metal fittings
  • Assemblies requiring immediate moderate-pressure sealing after tightening
Product Family

LOCTITE 542

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Dimethacrylate ester
Color
Brown liquid
Component System
One component
Specific Gravity
1.06
Thermal Properties
Linear thermal expansion
80×10^-6 K -1
Specific Heat Capacity
0.3 J/(g⋅°C)
Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity
400 to 800 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceBrown liquid-As supplied
Chemical typeDimethacrylate ester-One-component material
Specific gravity1.06-25 deg C
Viscosity1,200 to 2,750mPa sBrookfield RVT, spindle 2, 2.5 rpm, 25 deg C
Viscosity400 to 800mPa sBrookfield RVT, spindle 2, 20 rpm, 25 deg C
Viscosity150mPa sEN 12092-MV, 277 s^-1, 25 deg C
Flow behaviorThixotropic-As supplied
Cure mechanismAnaerobic-Confined between close-fitting metal threads
Technical properties

After-processing / final-state properties

Typical values for the cured, bonded, treated, or in-service product under the listed conditions.

PropertyValueUnitMethod / condition
Breakaway torque15N mM10 steel nuts and bolts, cured 24 h at 22 deg C
Prevailing torque9N mM10 steel nuts and bolts, cured 24 h at 22 deg C
Breakloose torque after pretightening25N mM10 steel nuts and bolts, pretightened to 5 N m, cured 24 h at 22 deg C
Maximum prevailing torque after pretightening25N mM10 steel nuts and bolts, pretightened to 5 N m, cured 24 h at 22 deg C
Compressive shear strength>=6.5N/mm^2Steel pins and collars, cured 24 h at 22 deg C
Maximum pressure / solvent-resistance development24hMinimum recommended cure after assembly

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers