LOCTITE 5240

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE 5240 LOCTITE 5240 LOCTITE 5240

Main features

  • Light-and-Moisture Dual Cure
  • Shear-Thinning Cavity Filling
  • Flexible Electrically Insulating Rubber

Product Description

LOCTITE SI 5240 is a clear, flowable one-component alkoxy silicone for bonding, potting, coating, and sealing. UV or visible light rapidly cures exposed material, while atmospheric moisture provides secondary cure in shadowed regions. The shear-thinning liquid supports controlled dispensing and uniform cavity filling before forming a flexible silicone rubber. Typical cured properties include Shore A hardness of at least 40, tensile strength of at least 3 N/mm^2, and elongation from 250% to 450% at the specified cure condition. Full ambient property development occurs over approximately 72 hours.

Key features

  • Light-and-moisture dual cure: Exposed material cures with UV or visible light, while atmospheric moisture supports shadowed regions.
  • Shear-thinning cavity flow: The 15,000 to 35,000 mPa s liquid supports controlled dispensing and uniform filling.
  • Flexible insulating silicone: The cured rubber combines high elongation with measured dielectric and mechanical properties.

Applications / Suitable for

  • Bonding and sealing components
  • Potting and cavity filling
  • Protective coating of assemblies
Product Family

LOCTITE 5240

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Alkoxy silicone
Color
Clear liquid with yellow to green tint slight haze permissible
Component System
One component
Specific Gravity
1.06
Physical Properties
Depth of Cure
≥10 mm
Tack-Free Time
50 to 55 minutes
Viscosity
15,000 to 35,000 mPa.s
Mechanical Properties
Elongation
250 to 450 %
Electrical Properties
Dielectric Strength
21 kV/mm
Surface Resistivity
5.15×10^15 Ohms/sq
Volume Resistivity
1.2×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
5 to 10 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceClear with yellow-green tint-As supplied
Chemical typeAlkoxy silicone-One-component material
Specific gravity1.06-23 deg C
Viscosity15,000 to 35,000mPa sBrookfield RVT, spindle 5, 10 rpm, 25 deg C
Flow behaviorShear thinning-Thixotropic as supplied
Primary cure mechanismUV / visible light-Exposed material
Secondary cure mechanismAtmospheric moisture-Shadowed regions
Technical properties

After-processing / final-state properties

Typical values for the cured, bonded, treated, or in-service product under the listed conditions.

PropertyValueUnitMethod / condition
Shore hardness>=40Shore A70 mW/cm^2 at 365 nm for 60 s per side, then 7 d at 22 deg C
Elongation at break250 to 450%70 mW/cm^2 at 365 nm for 60 s per side, then 7 d at 22 deg C
Tensile strength>=3N/mm^270 mW/cm^2 at 365 nm for 60 s per side, then 7 d at 22 deg C
Tensile modulus at 100% strain1N/mm^270 mW/cm^2 at 365 nm for 60 s per side, then 7 d at 22 deg C
Tear strength12.6N/mm70 mW/cm^2 at 365 nm for 60 s per side, then 7 d at 22 deg C
Volume shrinkage0.8%Cured material
Dielectric breakdown strength21kV/mmCured material
Volume resistivity1.2 x 10^15ohm cmCured material

Leading Brands Trust in Our Products and Services