LOCTITE 5188

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 5188

Main features

  • Flexible Cured Sealing
  • Strong Aluminum Adhesion
  • High-Viscosity Placement Control

Product Description

LOCTITE® 5188™ is a single-component, medium-strength anaerobic form-in-place gasketing product for close-fitting rigid metal flange connections. It cures between mating metal surfaces in the absence of air and is particularly suited to aluminum substrates. The flexible formulation maintains flexibility after high-temperature exposure, tolerates minor oil contamination on flange surfaces, and provides resistance to low pressures immediately after assembly. Typical uses include sealing gearboxes, engine casings, and other rigid metal flanged assemblies.

Key features

  • Flexible flange sealing: Maintains flexibility after exposure to elevated temperatures.
  • Aluminum performance: Provides strong adhesion on close-fitting aluminum flange surfaces.
  • One-component application: Requires no mixing and can be dispensed manually or with automated equipment.
Product Family

LOCTITE 5188

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red viscous product
Specific Gravity
1.1
Physical Properties
Viscosity
11,000 - 32,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
105 °C
Mechanical Properties
Elongation
186 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Dimethacrylate ester — Uncured material
Appearance Red viscous product — Uncured material
Components One component — No mixing required
Fluorescence Positive — Under ultraviolet light
Specific gravity 1.1 — At 25°C
Viscosity 11,000–32,000 mPa·s Cone and plate, 25°C; PK 100, PK 1, 2° cone at 20 s⁻¹
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, specimen, and test method.

Property Value Unit Method / condition
Glass-transition temperature 105 °C Typical cured-material property
Elongation at break 186 % Typical cured-material property
Tensile strength at break 4.24 N/mm² Typical cured-material property
Tensile modulus 4.17 N/mm² Typical cured-material property
Lap-shear strength 9.2 N/mm² Grit-blasted mild steel; cured 72 hours at 22°C
Lap-shear strength 7.0 N/mm² Aluminum; cured 72 hours at 22°C
Lap-shear strength 7.8 N/mm² Grit-blasted mild steel; cured 168 hours at 22°C
Lap-shear strength 8.0 N/mm² Aluminum; cured 168 hours at 22°C
Maximum sealed induced gap 0.25 mm Annular gasket on mild steel; tested to 1.3 MPa after curing