LOCTITE 518

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 518

Main features

  • Anaerobic Thread Sealing
  • Gap-Filling Sealant Formulation
  • Thixotropic Application Control

Product Description

LOCTITE® 518™ is a single-component, medium-strength anaerobic flange sealant formulated for close-fitting rigid metal surfaces. The thixotropic red acrylic material cures when confined between mating metal faces in the absence of air and provides resistance to low pressures immediately after flange assembly. It seals gaps up to 0.25 mm and tolerates minor surface contamination from oils, including lubricating, anti-corrosion, and protection fluids. Typical uses include form-in-place gasketing of rigid metal flanges and casings, such as gearbox and engine assemblies.

Key features

  • Anaerobic flange sealing: Cures between close-fitting metal surfaces when isolated from air.
  • Gap-filling capability: Designed for flanged parts with gaps up to 0.25 mm.
  • Thixotropic consistency: Helps limit migration of the uncured material after application.
Product Family

LOCTITE 518

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red gel-like material
Specific Gravity
1.1
Physical Properties
Viscosity
4,000,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
100 °C
Mechanical Properties
Elongation
64 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Dimethacrylate ester — Uncured material
Appearance Red gel-like material — Uncured material
Fluorescence Positive — Under ultraviolet light
Specific gravity 1.1 — At 23°C
Viscosity 4,000,000 mPa·s Brookfield HBT, 25°C; spindle TC, 0.5 rpm, Helipath
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, specimen, and test method.

Property Value Unit Method / condition
Glass-transition temperature 100 °C ISO 11359-2; cured 24 hours at 23°C
Elongation at break 64 % ISO 527-2; cured 24 hours at 23°C
Tensile strength 7.3 N/mm² ISO 527-2; cured 24 hours at 23°C
Tensile modulus 54 N/mm² ISO 527-2; cured 24 hours at 23°C
Compressive shear strength 5 N/mm² ISO 10123; steel pins and collars; cured 24 hours at 23°C
Lap-shear strength 8.4 N/mm² ISO 4587; grit-blasted mild steel; cured 24 hours at 23°C
Maximum sealed induced gap 0.25 mm Annular gasket; mild steel or aluminum; cured 20 hours at room temperature