LOCTITE 5056

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

LOCTITE 5056 LOCTITE 5056

Main features

  • Rapid UV Silicone Cure
  • Low-Viscosity Potting and Coating
  • Transparent Elastomeric Final State

Product Description

LOCTITE SI 5056 is a light-yellow, transparent, one-component alkoxy silicone adhesive for UV and visible-light curing in bonding, potting, coating, and sealing applications. The low-viscosity liquid cures to a tough, transparent silicone rubber for assemblies requiring a flexible, electrically insulating final material. Under the specified 365 nm exposure, the surface can become tack free within 30 seconds and cure to a depth of at least 4 mm in 60 seconds. Disposable medical-device assembly is included within the product-specific ISO 10993-based evaluation scope.

Key features

  • Rapid light-cure processing: The surface becomes tack free within 30 seconds under the documented 365 nm exposure.
  • Low-viscosity multi-function application: The liquid supports bonding, potting, coating, and sealing before light cure.
  • Transparent elastomeric final state: The cured silicone combines transparency, Shore A hardness of 35 to 50, and elongation above 170%.

Applications / Suitable for

  • Bonding, potting, coating, and sealing
  • Disposable medical-device assembly within documented evaluation scope
  • Light-accessible assemblies requiring transparent cured silicone
Product Family

LOCTITE 5056

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Alkoxy silicone
Color
Light yellow, transparent liquid
Component System
One component
Specific Gravity
0.98
Physical Properties
Depth of Cure
≥4 mm
Tack-Free Time
75 minutes
Viscosity
1,400 to 3,000 mPa.s
Mechanical Properties
Elongation
>170 %
Electrical Properties
Dielectric Strength
22.8 kV/mm
Volume Resistivity
9.9×10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceLight yellow, transparent liquid-Uncured
Chemical typeAlkoxy silicone-As supplied
ComponentsOne component-No mixing required
Specific gravity0.98-As supplied
Viscosity1,400 to 3,000mPa sBrookfield RVT, spindle 3, 20 rpm, 25 deg C
Cure mechanismUV / visible light-Light-initiated cure
Primary functionsBonding, potting, coating, sealing-As supplied product positioning
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Tack-free time<=30sZeta 7215, 70 mW/cm^2 measured at 365 nm
Depth of cure>=4mm70 mW/cm^2 at 365 nm for 60 s, Zeta 7200
Shore hardness35 to 50Shore AISO 868; cured 70 mW/cm^2 at 365 nm for 60 s
Elongation at break>170%ISO 527-3; cured 70 mW/cm^2 at 365 nm for 60 s
Tensile strength>5.0N/mm^2ISO 527-3; cured 70 mW/cm^2 at 365 nm for 60 s
Dielectric breakdown strength22.8kV/mmIEC 60243-1; light cured per listed condition plus 24 h at 22 deg C, 50% RH
Lap shear, UV-transmitting polycarbonate4N/mm^2Polycarbonate to polycarbonate; light cured 60 s per side plus 24 h at 22 deg C, 50% RH