LOCTITE 5045

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE 5045

Main features

  • Non-Slumping RTV Application
  • Flexible Shock-Absorbing Silicone
  • Strain-Relief Component Reinforcement

Product Description

LOCTITE SI 5045 is a translucent, non-slumping, one-component alkoxy RTV silicone paste for bonding, sealing, and coating components. It cures at room temperature through atmospheric moisture and requires no mixing. The paste format supports reinforcement and strain relief around delicate parts while limiting flow away from the applied area. The cured silicone combines low Shore A hardness, high elongation, and measured tensile and tear properties for a flexible final state. It resists weathering, moisture, and ozone and is used in industrial, military, and automotive assemblies within its stated application and temperature limits.

Key features

  • Non-slumping RTV placement: The paste remains positioned for bonding, sealing, coating, and reinforcement around components.
  • Flexible strain-relief material: A Shore A hardness of 25 and 500% elongation support a compliant cured silicone state.
  • Environmental silicone resistance: The cured material is documented for weathering, moisture, and ozone exposure within its application scope.

Applications / Suitable for

  • Bonding, sealing, and coating components
  • Strain relief and reinforcement of delicate parts
  • Industrial, military, and automotive component assemblies
Product Family

LOCTITE 5045

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Alkoxy silicone
Color
Translucent paste
Component System
One component
Solids
92 %
Specific Gravity
1.14
Thermal Properties
Linear thermal expansion
3×10^-4 K -1
Thermal Conductivity
0.2 W/m.K
Physical Properties
Extrusion Rate
40 g/min
Tack-Free Time
300 minutes
Viscosity
Paste mPa.s
Chemical Properties
Water Absorption
0.01 %
Mechanical Properties
Elongation
500 %
Peel Strength
13 N/mm
Electrical Properties
Dielectric Strength
18 kV/mm
Volume Resistivity
4×10^15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceTranslucent paste-Uncured
Chemical typeAlkoxy silicone-As supplied
ComponentsOne component-No mixing required
Specific gravity1.14-23 deg C
Solids / non-volatile content92%As supplied
Extrusion rate40g/min0.62 MPa for 15 s at 25 deg C, Semco cartridge
Cure mechanismRoom-temperature vulcanizing-Atmospheric-moisture cure
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Tack-free time5h23 deg C, 50% RH
Full performance development72hRoom-temperature moisture cure
Shore hardness25Shore AISO 868; cured 1 week at 23 deg C, 50% RH
Elongation at break500%ISO 37; cured 1 week at 23 deg C, 50% RH
Tensile strength3N/mm^2ISO 37; cured 1 week at 23 deg C, 50% RH
Tear strength40N/mmISO 34-1, die B; cured 1 week at 23 deg C, 50% RH
Water absorption0.01%ISO 62; 24 h in water at 23 deg C
Dielectric breakdown strength18kV/mmIEC 60243-1; cured 1 week at 23 deg C, 50% RH