LOCTITE 498

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE 498

Main features

  • General-Purpose Cyanoacrylate Adhesive
  • Cured Thermal-Cycling Resistance
  • Cured Humidity Resistance

Product Description

LOCTITE® 498™ is a one-component, medium-viscosity ethyl cyanoacrylate adhesive designed for general-purpose bonding applications requiring elevated temperature resistance and excellent humidity durability. The adhesive rapidly bonds metals, plastics and elastomers through moisture curing and is formulated to withstand thermal cycling while maintaining reliable bond strength. Its combination of fast fixture speed, high glass transition temperature and good environmental resistance makes it suitable for demanding industrial assembly applications where long-term performance under heat exposure is required.

  • General-purpose cyanoacrylate adhesive with enhanced heat resistance.
  • Excellent resistance to thermal cycling.
  • Superior humidity resistance compared with standard formulations.
  • Rapid humidity-cure technology.
  • One-component system requiring no mixing.
  • Bonds rubbers, plastics and metals.
  • Suitable for applications requiring elevated-temperature performance.

Recommended Applications

  • General industrial bonding operations.
  • Assemblies exposed to heat and thermal cycling.
  • Bonding metals, rubbers and engineering plastics.
  • Applications requiring humidity resistance.
  • Precision assembly with close-fitting bond lines.
Product Family

LOCTITE 498

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent, colorless to pale yellow liquid
Specific Gravity
1.1
Physical Properties
Viscosity
400 - 600 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
120 °C
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Volume Resistivity
10e+15 Ohms⋅cm

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Heat-resistant instant adhesive
Chemical Type Ethyl Cyanoacrylate — One-component formulation
Appearance Transparent, Colorless to Pale Yellow Liquid — Uncured material
Components One Part — No mixing required
Specific Gravity 1.10 — 25°C
Viscosity 400 - 600 mPa·s (cP) Brookfield LVF, Spindle 2, 30 rpm, 25°C
Key Substrates Rubbers, Plastics, Metals — Recommended bonding materials
Cure Mechanism Humidity Cure — Atmospheric moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 120 °C ASTM E228
Coefficient of Thermal Expansion 80 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.10 W/(m·K) ISO 8302
Volume Resistivity 10 × 10¹⁵ Ω·cm IEC 60093
Dielectric Breakdown Strength 25 kV/mm IEC 60243-1
Dielectric Constant / Dissipation Factor 2.3 / <0.02 — 0.05 kHz to 1,000 kHz
Lap Shear Strength (Steel) 19 N/mm² ISO 4587, 24 h cure at 22°C
Lap Shear Strength (Polycarbonate) 10 N/mm² ISO 4587, 24 h cure
Lap Shear Strength (Phenolic) 10 N/mm² ISO 4587, 24 h cure
Heat-Aged Lap Shear Strength (Steel) ≥6.9 N/mm² After 24 h cure + 24 h at 121°C, tested at 121°C
Initial Lap Shear Strength (Steel) ≥4.8

Leading Brands Trust in Our Products and Services