Loctite 495

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite 495

Main features

  • One-Part Adhesive Form
  • Multi-Substrate Assembly Fixturing
  • Low-Viscosity Adhesive Application

Product Description

LOCTITE® 495 Instant Adhesive is a one-part, low-viscosity ethyl cyanoacrylate adhesive designed for rapid bonding of plastics, rubbers, and metals. Atmospheric moisture initiates the cure, allowing closely fitted components to fixture within seconds depending on the substrate, bond gap, humidity, and ambient conditions.

Key features

  • One-part cyanoacrylate: Requires no mixing and cures through exposure to atmospheric moisture.
  • Rapid fixture: Typical fixture times range from less than 5 seconds to 15 seconds on documented substrates at 22 °C and 50% relative humidity.
  • Low-viscosity liquid: Typical cone-and-plate viscosity is 20 to 45 mPa·s at 25 °C and a shear rate of 3,000 s-1.

Applications / Suitable for

  • Bonding closely fitted plastic components
  • Bonding rubber and elastomer components
  • Rapid bonding of metal components
Product Family

LOCTITE 495

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent
Chemistry Type
Ethyl Cyanoacrylate

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured adhesive. Values are not guaranteed production specifications unless identified as controlled limits.

Property Value Unit Method / condition
Chemical type Ethyl cyanoacrylate — As supplied
Appearance Transparent, colorless to straw-colored liquid — Uncured
Specific gravity 1.1 — At 25 °C
Viscosity 20–45 mPa·s (cP) Cone and plate; 25 °C; shear rate 3,000 s-1
Viscosity 20–60 mPa·s (cP) Brookfield LVF; spindle 1; 30 rpm; 25 °C
Technical properties

After-processing / final-state properties

Typical adhesive-strength results after curing for 24 hours at 22 °C. Performance depends on substrate, preparation, bond geometry, cure conditions, and test configuration.

Property Value Unit Method / condition
Lap shear strength — steel 14.2 N/mm² ISO 4587; grit-blasted steel; 24 hours at 22 °C
Lap shear strength — aluminum 10.8 N/mm² ISO 4587; grit-blasted aluminum; 24 hours at 22 °C
Lap shear strength — ABS 7.9 N/mm² ISO 4587; 24 hours at 22 °C; substrate failure reported
Lap shear strength — PVC 8.7 N/mm² ISO 4587; 24 hours at 22 °C; substrate failure reported
Tensile strength — Buna-N 13.7 N/mm² ISO 6922; 24 hours at 22 °C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers