LOCTITE 493

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 493

Main features

  • Very-Low-Viscosity Capillary Bonding
  • Fast Metal-Focused Fixturing
  • Broad Rubber-Plastic Bonding

Product Description

LOCTITE 493 is a clear to slightly hazy, very-low-viscosity methyl cyanoacrylate instant adhesive for general-purpose bonding, with particular suitability for metals. The one-part liquid also bonds supported rubber and plastic substrates and cures through atmospheric moisture without mixing. A cone-and-plate viscosity of 1 to 4 mPa s supports capillary flow into very close-fitting joints. Fixture time ranges from under 10 seconds on neoprene and nitrile rubber to 20 to 60 seconds on tested metals under the specified conditions. Full chemical and solvent resistance develops after at least 24 hours.

Key features

  • Very-low-viscosity capillary flow: A 1 to 4 mPa s viscosity supports penetration into very close-fitting bondlines.
  • Metal-focused instant bonding: The methyl cyanoacrylate formulation is particularly suited to rapid metal assembly.
  • Fast rubber and plastic fixture: Tested elastomers fixture in under 10 seconds, with short fixture times on ABS and other plastics.

Applications / Suitable for

  • Capillary bonding of close-fitting metal joints
  • Rapid rubber and elastomer bonding
  • General-purpose plastic assembly
Product Family

LOCTITE 493

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methyl cyanoacrylate
Color
Clear to slightly hazy, colorless liquid
Component System
One component
Specific Gravity
1.1
Thermal Properties
Linear thermal expansion
100x10^-6 K -1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity
1 to 10 mPa.s
Mechanical Properties
Peel Strength
<0.5 N/mm
Electrical Properties
Dielectric Strength
25 kV/mm
Surface Resistivity
10×10^15 to 80×10^15 Ohms/sq
Volume Resistivity
2×10^15 to 10×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
20 to 40 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceClear to slightly hazy, colorless liquid-Uncured
Chemical typeMethyl cyanoacrylate-As supplied
ComponentsOne part-No mixing required
Specific gravity1.1-25 deg C
Viscosity1 to 4mPa sCone and plate, 25 deg C, shear rate 3,000 s^-1
Viscosity1 to 10mPa sBrookfield LVF, spindle 1, 60 rpm, 25 deg C
Vapor pressure<1hPaAs supplied
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time, degreased mild steel20 to 40s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, nitrile rubber<10s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, ABS10 to 30s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Coefficient of thermal expansion100 x 10^-6K^-1ISO 11359-2; after 24 h at 22 deg C
Lap shear strength, grit-blasted steel20 to 30N/mm^2ISO 4587; cured 24 h at 22 deg C
Lap shear strength, grit-blasted aluminum15 to 22N/mm^2ISO 4587; cured 24 h at 22 deg C
Dielectric breakdown strength25kV/mmIEC 60243-1; after 24 h at 22 deg C