LOCTITE 4861

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 4861

Main features

  • Flexible Cured Adhesive
  • Rapid Humidity Cure
  • Medium-Viscosity Application Control

Product Description

LOCTITE® 4861™ is a one-component ethyl/butyl cyanoacrylate adhesive specifically formulated to create flexible bond lines while maintaining rapid curing performance. The medium-viscosity adhesive is designed for bonding difficult-to-bond materials including metals, plastics and elastomers, and is especially effective when joining rubber components where joint compressibility must be maintained. It also performs well on porous and absorbent substrates such as paper, leather and fabrics. LOCTITE 4861 has been evaluated to Henkel test protocols based on ISO 10993 biocompatibility standards and is suitable for use in disposable medical device assembly applications.

Key Features & Benefits

  • Flexible bond-line formulation for improved joint performance.
  • Rapid humidity-cure cyanoacrylate technology.
  • Maintains compressibility in bonded rubber assemblies.
  • Suitable for metals, plastics, elastomers and porous materials.
  • Medium viscosity for controlled application.
  • One-component formulation requiring no mixing.
  • Evaluated to ISO 10993-based biocompatibility protocols for medical device use.

Recommended Applications

  • Disposable medical device assembly.
  • Rubber-to-metal and rubber-to-plastic bonding.
  • Flexible bonding applications requiring shock absorption.
  • Bonding paper, leather and fabric materials.
  • General industrial assembly of metals, plastics and elastomers.
Product Family

LOCTITE 4861

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear colorless liquid
Specific Gravity
1.05
Physical Properties
Viscosity
3,000 - 5,500 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
60 °C
Electrical Properties
Surface Resistivity
1e+15 Ohms/sq
Volume Resistivity
158e+12 Ohms⋅cm

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Flexible instant adhesive
Chemical Type Ethyl / Butyl Cyanoacrylate — Flexible bonding formulation
Appearance Clear Colorless Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.05 — 25°C
Viscosity 3,000 - 5,500 mPa·s (cP) Cone & Plate, 25°C, 50 s⁻¹
Key Substrates Steel, Polycarbonate, ABS — Typical bonding materials
Cure Mechanism Humidity Cure — Atmospheric moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 60 °C ASTM E228
Coefficient of Thermal Expansion 100 × 10⁻⁶ K⁻¹ ISO 11359-2
Shore Hardness 80 - 90 Shore A ISO 868
Tensile Modulus 280 - 580 N/mm² ISO 527-3
Volume Resistivity 158 × 10¹² Ω·cm IEC 60093
Surface Resistivity >1 × 10¹⁵ Ω IEC 60093
Lap Shear Strength (Steel) 11 - 17 N/mm² ISO 4587, 7 days cure
Lap Shear Strength (Aluminum) 8 - 12 N/mm² ISO 4587, grit blasted
Lap Shear Strength (ABS) 5 - 9 N/mm² ISO 4587
Lap Shear Strength (Polycarbonate) 6 - 8 N/mm² ISO 4587

Leading Brands Trust in Our Products and Services