LOCTITE 460

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 460

Main features

  • Low-Odor Low-Blooming Cure
  • Very Fast Porous-Substrate Fixturing
  • Low-Viscosity Vapor-Controlled Bonding

Product Description

LOCTITE 460 is a transparent, low-viscosity alkoxyethyl cyanoacrylate instant adhesive with low-odor and low-blooming characteristics. The one-part liquid bonds metals, plastics, elastomers, and porous or absorbent materials and is particularly relevant where vapor control is difficult. A viscosity of 25 to 55 mPa s supports rapid wetting and thin bondlines. Fixture time can be under 5 seconds on ABS, nitrile rubber, neoprene, phenolic, or paper, with longer times on some metals and plastics. Full chemical and solvent resistance develops after at least 24 hours.

Key features

  • Low-odor low-blooming cure: The alkoxyethyl cyanoacrylate chemistry limits odor and visible blooming where vapor control is difficult.
  • Rapid porous-material fixture: Paper and several other tested substrates fixture in less than 5 seconds under documented conditions.
  • Low-viscosity thin-gap flow: A 25 to 55 mPa s viscosity supports fast wetting of close-fitting assemblies.

Applications / Suitable for

  • Bonding where odor and blooming control are important
  • Rapid assembly of metals, plastics, and elastomers
  • Bonding wood, paper, leather, and fabric
Product Family

LOCTITE 460

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Alkoxyethyl cyanoacrylate
Color
Transparent, colorless to straw colored liquid
Component System
One component
Specific Gravity
1.1
Physical Properties
Viscosity
30 to 50 mPa.s
Curing Conditions
Fixture Time
10 to 30 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to straw liquid-Uncured
Chemical typeAlkoxyethyl cyanoacrylate-As supplied
ComponentsOne part-No mixing required
Specific gravity1.1-25 deg C
Viscosity25 to 55mPa sCone and plate, 25 deg C, shear rate 3,000 s^-1
Viscosity30 to 50mPa sBrookfield LVF, spindle 1, 30 rpm, 25 deg C
Cure mechanismHumidity-Atmospheric moisture
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time, ABS<5s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, steel10 to 30s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, aluminum5 to 10s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Tensile strength, Buna-N>=4.5N/mm^2ISO 6922; cured 10 s at 22 deg C
Lap shear strength, grit-blasted steel21N/mm^2ISO 4587; cured 72 h at 22 deg C
Lap shear strength, etched aluminum18N/mm^2ISO 4587; cured 72 h at 22 deg C
Lap shear strength, polycarbonate7.7N/mm^2ISO 4587; cured 72 h at 22 deg C

Leading Brands Trust in Our Products and Services