LOCTITE 454

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 454

Main features

  • Thixotropic Application Control
  • High-Strength Structural Bonding
  • Moisture-Cure Bonding Processing

Product Description

LOCTITE® 454™ is a one-component, high-viscosity thixotropic ethyl cyanoacrylate adhesive designed for bonding difficult-to-bond materials requiring uniform stress distribution and strong tensile and shear strength. Its gel consistency prevents running and dripping, making it ideal for vertical and overhead applications. The adhesive rapidly bonds metals, plastics and elastomers, while also performing well on porous substrates such as wood, paper, leather and fabric. LOCTITE 454 cures in the presence of atmospheric moisture and develops high strength with excellent environmental resistance.

Key Features & Benefits

  • Thixotropic gel formulation prevents adhesive flow and dripping.
  • High-strength bonding for metals, plastics and elastomers.
  • Suitable for porous materials including wood, paper, leather and fabric.
  • One-part adhesive requiring no mixing.
  • Rapid moisture-cure cyanoacrylate technology.
  • Good tensile, shear and environmental resistance properties.
  • Effective on vertical and overhead bonding applications.

Recommended Applications

  • Bonding difficult-to-bond substrates requiring stress distribution.
  • Vertical and overhead assembly applications.
  • Metal, plastic and elastomer assembly.
  • Wood, paper, leather and fabric bonding.
  • General industrial maintenance and repair operations.
Product Family

LOCTITE 454

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear to slightly cloudy gel
Specific Gravity
1.1
Physical Properties
Viscosity
150 - 450 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Ethyl cyanoacrylate adhesive
Chemical Type Ethyl Cyanoacrylate — One-part formulation
Appearance Clear to Slightly Cloudy Gel — Uncured material
Specific Gravity 1.10 — 25°C
Casson Viscosity 150 - 450 mPa·s (cP) Cone & Plate Rheometer, 25°C
Brookfield Viscosity 18,000 - 40,000 mPa·s (cP) RVT, Spindle TC, 20 rpm, 25°C
Viscosity Characteristic High, Thixotropic — Gel consistency
Cure Mechanism Humidity Cure — Atmospheric moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Tensile Strength (Buna-N) 15.1 N/mm² ISO 6922, 72 h cure at 22°C
Lap Shear Strength (Steel) 20.9 N/mm² ISO 4587, grit blasted steel
Lap Shear Strength (Aluminum) 17.1 N/mm² ISO 4587, etched aluminum
Lap Shear Strength (Polycarbonate) 7.7 N/mm² ISO 4587
Block Shear Strength (ABS) 23.3 N/mm² ISO 13445
Block Shear Strength (Polycarbonate) 9.6 N/mm² ISO 13445
Relative Humidity Resistance 55% Retention After 1,000 h at 98% RH, 40°C
Water Resistance 75% Retention After 1,000 h water immersion at 22°C
Ethanol Resistance 120% Retention After 1,000 h exposure at 22°C