LOCTITE 444

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 444

Main features

  • TAK PAK Accelerator Compatibility
  • One-Component Cyanoacrylate Adhesive
  • Documented A-A-3097 Qualification

Product Description

LOCTITE® 444™ is a one-component, medium-viscosity ethyl cyanoacrylate adhesive specifically formulated for electronics assembly applications. It provides rapid room-temperature curing through reaction with atmospheric moisture and is designed for use with LOCTITE® TAK PAK® accelerators to achieve instant fixturing when required. The adhesive bonds plastics, rubbers and metals, making it suitable for wire tacking, tamper-proofing adjustable components, attaching edge guides and mounting standoffs or stiffeners onto circuit boards. Its medium viscosity ensures controlled application while delivering strong, reliable bonding performance in demanding electronic manufacturing environments.

Key Features & Benefits

  • Single-component adhesive requiring no mixing.
  • Fast moisture-cure cyanoacrylate technology.
  • Medium viscosity enables controlled dispensing and positioning.
  • Compatible with LOCTITE® TAK PAK® accelerators for instant cure.
  • Bonds plastics, rubbers and metals.
  • Designed for electronics manufacturing applications.
  • Qualified to Commercial Item Description A-A-3097.

Recommended Applications

  • Wire tacking to coil forms.
  • Tamper-proofing adjustable electronic components.
  • Mounting standoffs and edge guides on circuit boards.
  • Attaching stiffeners to printed circuit boards.
  • General bonding of plastics, metals and elastomers.
Product Family

LOCTITE 444

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless transparent liquid
Specific Gravity
1.050
Physical Properties
Viscosity
550 - 850 mPa.s