LOCTITE 438

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 438

Main features

  • Black Rubber-Toughened Bonding
  • Enhanced Shock and Peel Resistance
  • Low-Viscosity Multi-Material Assembly

Product Description

LOCTITE 438 is a black, one-part, low-viscosity, rubber-toughened ethyl cyanoacrylate instant adhesive for bonding metals, plastics, rubbers, and selected porous materials. Its black color makes adhesive placement visible, while the toughened formulation combines increased flexibility and peel strength with resistance to shock. A viscosity of 100 to 250 mPa s supports thin bondlines and rapid wetting. Fixture time ranges from under 5 seconds on nitrile rubber and balsa wood to 30 to 60 seconds on common metal substrates under the specified conditions.

Key features

  • Black visible bondline: The black liquid provides clear visual contrast for adhesive placement and cured bond identification.
  • Rubber-toughened performance: Increased flexibility and peel strength are combined with enhanced resistance to shock.
  • Low-viscosity multi-material cure: A 100 to 250 mPa s viscosity supports rapid bonding across tested metals, plastics, rubbers, and porous materials.

Applications / Suitable for

  • Visible black bonding of metals and plastics
  • Shock- and peel-resistant rubber bonding
  • Bonding selected wood, paper, leather, and fabric
Product Family

LOCTITE 438

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate
Color
Black liquid
Component System
One component
Specific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg)
130 °C
Linear thermal expansion
80x10^-6 K -1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity
100 to 250 mPa.s
Mechanical Properties
Peel Strength
4 N/mm
Electrical Properties
Dielectric Strength
25 kV/mm
Surface Resistivity
10×10^15 Ohms Ohms/sq
Volume Resistivity
10×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
30 to 45 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceBlack liquid-Uncured
Chemical typeEthyl cyanoacrylate-As supplied
ComponentsOne part-No mixing required
Specific gravity1.1-25 deg C
Viscosity100 to 250mPa sCone and plate, 25 deg C, shear rate 1,000 s^-1
Cure mechanismHumidity-Atmospheric moisture
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time, nitrile rubber<5s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, ABS10 to 20s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, aluminum<=60sIsopropanol-wiped aluminum, 22 deg C, 50% RH
Glass transition temperature130deg CISO 11359-2; cured 24 h at 22 deg C
Lap shear strength, grit-blasted steel19N/mm^2ISO 4587; cured 24 h at 22 deg C
180-degree peel strength, grit-blasted steel4N/mmISO 8510-2; cured 48 h at 22 deg C
Side impact resistance, aluminum>=4JCured 24 h at 22 deg C

Leading Brands Trust in Our Products and Services