LOCTITE 435

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 435 LOCTITE 435

Main features

  • Rubber-Toughened Peel Resistance
  • Low-Viscosity Rapid Bonding
  • Porous-Material Bonding Range

Product Description

LOCTITE 435 is a one-part, low-viscosity, rubber-toughened ethyl cyanoacrylate instant adhesive for metals, plastics, rubbers, and selected porous materials. The toughened formulation combines increased flexibility and peel strength with resistance to shock. A viscosity of 100 to 250 mPa s supports rapid wetting and thin bondlines, while fixture time ranges from under 5 seconds on nitrile rubber and balsa wood to 30 to 60 seconds on common metal substrates. The adhesive also bonds wood, paper, leather, and fabric when those materials fit the assembly requirements.

Key features

  • Rubber-toughened flexibility: The cured adhesive provides increased flexibility and peel strength with enhanced shock resistance.
  • Low-viscosity rapid wetting: A 100 to 250 mPa s viscosity supports thin bondlines and fast fixture on many substrates.
  • Porous-material bonding range: The product supports selected wood, paper, leather, and fabric assemblies in addition to common engineering materials.

Applications / Suitable for

  • Shock- and peel-resistant bonding of metals
  • Bonding plastics, rubbers, and elastomers
  • Bonding selected porous or absorbent materials
Product Family

LOCTITE 435

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate with
Color
Colorless to straw colored, slightly cloudy liquid
Component System
One component
Specific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg)
130 °C
Linear thermal expansion
80x10^-6 K-1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity
100 to 250 mPa.s
Mechanical Properties
Peel Strength
4 N/mm
Electrical Properties
Dielectric Strength
25 kV/mm
Surface Resistivity
10×10^15 Ohms Ohms/sq
Volume Resistivity
10×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
30 to 45 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceColorless to straw, slightly cloudy liquid-Uncured
Chemical typeEthyl cyanoacrylate-As supplied
ComponentsOne part-No mixing required
Specific gravity1.1-25 deg C
Viscosity100 to 250mPa sCone and plate, 25 deg C, shear rate 1,000 s^-1
Cure mechanismHumidity-Atmospheric moisture
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time, nitrile rubber<5s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, ABS10 to 20s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, aluminum<=60sIsopropanol-wiped aluminum, 22 deg C, 50% RH
Glass transition temperature130deg CISO 11359-2; cured 24 h at 22 deg C
Lap shear strength, grit-blasted steel19N/mm^2Cured 24 h at 22 deg C
180-degree peel strength, grit-blasted steel4N/mmISO 8510-2; cured 48 h at 22 deg C
Side impact resistance, aluminum>=4JCured 24 h at 22 deg C