Main features

  • Low-Viscosity Dual Cure
  • Rapid Exposed-Surface Fixturing
  • Fluorescent Process Inspection

Product Description

LOCTITE 4310 is a one-part cyanoacrylate adhesive with UV and visible-light cure plus secondary humidity cure for plastics, rubbers, and metals. Its low-viscosity fluorescent liquid supports controlled dispensing and inspection of applied material. Exposed surfaces can reach tack-free cure in 5 seconds or less under several specified light sources, while humidity cure supports shadowed bond areas. Non-UV fixture times range from under 5 seconds on ABS to 20 to 30 seconds on degreased steel. It is suited to fast assembly processes that need rapid surface cure, thin adhesive flow, and a second cure mechanism.

Key features

  • Low-viscosity dual cure: A 100 to 250 mPa s liquid combines UV or visible-light cure with secondary humidity cure.
  • Rapid exposed-surface cure: Several documented light sources produce a tack-free surface in 5 seconds or less.
  • Fluorescent process inspection: Positive UV fluorescence supports visual confirmation of adhesive placement.

Applications / Suitable for

  • Rapid bonding of plastics, rubbers, and metals
  • Light curing of exposed adhesive surfaces and fillets
  • Disposable medical-device assembly within documented evaluation scope
Product Family

LOCTITE 4310

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate with photoinitiator
Color
Transparent, light yellow-green to dark blue-green liquid
Component System
One component
Specific Gravity
1.06
Thermal Properties
Glass Transition Temperature (Tg)
102 °C
Linear thermal expansion
56x10^-6 K -1
Physical Properties
Tack-Free Time
≤10 minutes
Viscosity
100 to 250 mPa.s
Chemical Properties
Water Absorption
2.2 %
Mechanical Properties
Elongation
7.3 %
Peel Strength
3 N/mm
Electrical Properties
Volume Resistivity
10.9×10^15 Ohms⋅cm
Physical Properties
Depth of Cure
2 mm
Curing Conditions
Fixture Time
5 to 15 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceLight yellow-green to dark blue-green liquid-As supplied
FluorescencePositive under UV light-As supplied
Chemical typeEthyl cyanoacrylate with photoinitiator-As supplied
ComponentsOne part-No mixing required
Specific gravity1.06-25 deg C
Viscosity100 to 250mPa sCone and plate, 25 deg C, shear rate 100 s^-1
Cure mechanismsUV / visible light; secondary humidity-Primary exposed-surface cure plus atmospheric-moisture cure
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Tack-free time<=5sZeta 7411-S, 30 mW/cm^2 measured at 365 nm
Fixture time, ABS<5sNon-UV cure, 22 deg C, 50% RH
Fixture time, degreased steel20 to 30sNon-UV cure, 22 deg C, 50% RH
Glass transition temperature102deg CASTM E 228; cured 100 mW/cm^2 at 365 nm for 30 s per side
Shore hardness84Shore DISO 868; cured 100 mW/cm^2 at 365 nm for 30 s per side
Tensile strength50N/mm^2ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side
Block shear, polycarbonate to polycarbonate22N/mm^2ISO 13445; cured 100 mW/cm^2 at 365 nm for 30 s

Leading Brands Trust in Our Products and Services