LOCTITE 431

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 431 LOCTITE 431 LOCTITE 431 LOCTITE 431

Main features

  • Medium-Viscosity Application Control
  • Rapid Multi-Material Bonding
  • Strong Shear-Oriented Performance

Product Description

LOCTITE 431 is a one-part, medium-viscosity ethyl cyanoacrylate instant adhesive for rapid bonding of metals, plastics, elastomers, and selected porous materials. Its viscosity range of 600 to 1,200 mPa s gives more placement control than very-low-viscosity grades while retaining quick fixture on many substrates. It is used in assemblies where uniform stress distribution and tension or shear performance are important. Fixture time varies with material, from 5 to 10 seconds on polycarbonate to 180 to 300 seconds on steel under the specified conditions. Full chemical and solvent resistance develops after at least 24 hours.

Key features

  • Medium-viscosity placement control: A 600 to 1,200 mPa s viscosity supports controlled dispensing while maintaining rapid cure.
  • Broad material bonding: The adhesive bonds tested metals, plastics, elastomers, and selected porous materials.
  • Strong shear-oriented performance: Documented steel and aluminum lap-shear values support evaluation for tension and shear-loaded joints.

Applications / Suitable for

  • Bonding metals, plastics, and elastomers
  • Assemblies requiring uniform stress distribution
  • Bonding wood, paper, leather, and fabric
Product Family

LOCTITE 431

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate
Color
Transparent, colorless to straw colored liquid
Component System
One component
Specific Gravity
1.07
Thermal Properties
Glass Transition Temperature (Tg)
183 °C
Linear thermal expansion
364x10^-6 K -1
Thermal Conductivity
0.3 W/m.K
Physical Properties
Viscosity
800 to 1,200 mPa.s
Electrical Properties
Dielectric Strength
25 kV/mm
Surface Resistivity
1.0×10^15 Ohms Ohms/sq
Volume Resistivity
10.9×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
180 to 300 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to straw liquid-Uncured
Chemical typeEthyl cyanoacrylate-As supplied
ComponentsOne part-No mixing required
Specific gravity1.07-25 deg C
Viscosity600 to 1,200mPa sCone and plate, 25 deg C, shear rate 3,000 s^-1
Viscosity800 to 1,200mPa sBrookfield LVF, spindle 2, 6 rpm, 25 deg C
Cure mechanismHumidity-Atmospheric moisture
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time, polycarbonate5 to 10s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, aluminum10 to 15s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, steel180 to 300s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Glass transition temperature183deg CISO 11359-2; cured 1 week at 22 deg C
Thermal conductivity0.3W/(m K)ISO 8302; cured 1 week at 22 deg C
Lap shear strength, grit-blasted steel25 to 31N/mm^2Cured 1 week at 22 deg C
Dielectric breakdown strength25kV/mmIEC 60243-1; cured 1 week at 22 deg C