LOCTITE 4307

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 4307 LOCTITE 4307 LOCTITE 4307

Main features

  • Rapid UV Surface Cure
  • Humidity Secondary Cure
  • Fluorescent Application Inspection

Product Description

LOCTITE 4307 is a one-part ethyl cyanoacrylate adhesive with UV and visible-light cure plus secondary humidity cure for plastics, rubbers, and metals. The fluorescent liquid supports application inspection, while exposed fillets and surfaces can reach a tack-free state in seconds under the specified light conditions. Humidity cure supports bonded interfaces outside direct light. A viscosity of 600 to 1,200 mPa s supports controlled placement, and non-UV fixture times range from 5 to 20 seconds on several tested substrates. It is suited to rapid assembly where fast fixturing and controlled exposed-surface cure are required.

Key features

  • Rapid light-cured surfaces: Exposed fillets and surfaces reach tack-free cure in 5 seconds or less with documented UV light sources.
  • Secondary humidity cure: Atmospheric moisture supports cure in bonded areas that do not receive direct light.
  • Fluorescent application inspection: Positive UV fluorescence helps operators identify applied adhesive during assembly.

Applications / Suitable for

  • Rapid bonding of plastics, rubbers, and metals
  • UV or visible-light curing of exposed fillets and surfaces
  • Disposable medical-device assembly within documented evaluation scope
Product Family

LOCTITE 4307

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate with photoinitiator
Color
Transparent, light yellow-green to dark blue-green liquid
Component System
One component
Specific Gravity
1.06
Thermal Properties
Glass Transition Temperature (Tg)
114 °C
Physical Properties
Tack-Free Time
≤5 seconds minutes
Viscosity
600 to 1,200 mPa.s
Chemical Properties
Water Absorption
2.6 %
Mechanical Properties
Elongation
2.2 %
Physical Properties
Depth of Cure
4 mm
Curing Conditions
Fixture Time
5 to 10 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceLight yellow-green to dark blue-green liquid-As supplied
FluorescencePositive under UV light-As supplied
Chemical typeEthyl cyanoacrylate with photoinitiator-As supplied
ComponentsOne part-No mixing required
Specific gravity1.06-25 deg C
Viscosity600 to 1,200mPa sCone and plate, 25 deg C, shear rate 100 s^-1
Cure mechanismsUV / visible light; secondary humidity-Primary exposed-surface cure plus atmospheric-moisture cure
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Tack-free time<=5sZeta 7400, 30 mW/cm^2 measured at 365 nm
Fixture time, ABS5 to 10sNon-UV cure, 22 deg C, 50% RH
Fixture time, grit-blasted steel10 to 20sNon-UV cure, 22 deg C, 50% RH
Glass transition temperature114deg CASTM E 228; cured 100 mW/cm^2 at 365 nm for 30 s per side
Shore hardness82Shore DISO 868; cured 100 mW/cm^2 at 365 nm for 30 s per side
Tensile strength33.4N/mm^2ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side
Block shear, polycarbonate>=9.0N/mm^2ISO 13445; cured 30 mW/cm^2 at 365 nm for 10 s