LOCTITE 430

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 430

Main features

  • Low-Viscosity Metal Bonding
  • Fast Thin-Gap Fixturing
  • Broad Rubber-Plastic Compatibility

Product Description

LOCTITE 430 is a transparent, colorless, low-viscosity methyl cyanoacrylate instant adhesive for general-purpose bonding, with particular suitability for metal substrates. The one-part liquid also bonds supported rubber and plastic materials and cures through atmospheric moisture without mixing. Cone-and-plate viscosity of 60 to 90 mPa s supports thin bondlines and rapid wetting. Fixture time ranges from under 10 seconds on neoprene and nitrile rubber to 20 to 40 seconds on degreased steel under the specified conditions. Full chemical and solvent resistance develops after at least 24 hours.

Key features

  • Metal-focused instant bonding: The methyl cyanoacrylate formulation is particularly suited to close-fitting metal assemblies.
  • Low-viscosity thin-gap flow: A 60 to 90 mPa s cone-and-plate viscosity supports rapid wetting of narrow bondlines.
  • Fast multi-material fixture: Tested rubbers fixture in under 10 seconds, with short fixture times on metals and plastics.

Applications / Suitable for

  • Rapid bonding of close-fitting metal parts
  • Bonding supported rubber substrates
  • General-purpose plastic assembly
Product Family

LOCTITE 430

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methyl cyanoacrylate
Color
Transparent, colorless liquid
Component System
One component
Specific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg)
165 °C
Linear thermal expansion
100×10^-6 K -1
Thermal Conductivity
0.1 W/m.K
Physical Properties
Viscosity
70 to 110 mPa.s
Mechanical Properties
Peel Strength
<0.5 N/mm
Electrical Properties
Dielectric Strength
25 kV/mm
Surface Resistivity
10×10^15 Ohms Ohms/sq
Volume Resistivity
10×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
20 to 40 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless liquid-Uncured
Chemical typeMethyl cyanoacrylate-As supplied
ComponentsOne part-No mixing required
Specific gravity1.1-25 deg C
Viscosity60 to 90mPa sCone and plate, 25 deg C, shear rate 3,000 s^-1
Viscosity70 to 110mPa sBrookfield LVF, spindle 1, 30 rpm, 25 deg C
Cure mechanismHumidity-Atmospheric moisture
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time, degreased steel20 to 40s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, nitrile rubber<10s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, ABS10 to 30s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Glass transition temperature165deg CASTM E 228; cured 24 h at 22 deg C
Lap shear strength, grit-blasted steel20 to 30N/mm^2ISO 4587; cured 24 h at 22 deg C
Lap shear strength, grit-blasted aluminum15 to 22N/mm^2ISO 4587; cured 24 h at 22 deg C
Dielectric breakdown strength25kV/mmIEC 60243-1; cured 24 h at 22 deg C